Abstract (Originalsprache)
Lithium-sulfur batteries are a promising technology for next-generation energy storage due to their high theoretical specific capacity of 1675 mAh g -1 and high energy density of ~2600 Wh kg -1 . However, Li-S batteries suffer from lithium polysulfide (LiPS) shuttling, which involves insoluble species such as Li 2 S 2 and Li 2 S, a core degradation mechanism of Li-S secondary batteries. During cycling, soluble and insoluble LiPS dissolve in the electrolyte and migrate between the cathode and anode. The lack of operando tools capable of associating specific LiPS speciation with impedance evolution limits our understanding of Li-S interfacial kinetics, which is needed to support research on methods to eliminate LiPS shuttling. This work introduces a dual-modality characterization technique that synchronizes Raman and electrochemical impedance spectroscopy (EIS) measurements to detect soluble LiPS with the goal of identifying dynamic changes in interfacial resistance and kinetic reaction rates that correspond to specific stages of LiPS evolution. The Cathode Clarity battery uses a commercially available CR2032 case, modified with a non-traditional cathode and an 8 mm hole on the cathode case. The non-traditional cathode substrate is a stainless steel mesh that permits optical interrogation of the cathode surface, the electrolyte (LiTFSI salt in a 1:1 DOL/DME solvent mixture), and the separator. The cathode is fabricated by first dip-coating the mesh substrate with a primer, followed by the active material slurry. The active material slurry is a mixture of Super C65 conductive carbon, a polyethylene-based binder, and elemental sulfur in a 4:1:15 mass ratio. This characterization technique collects Raman and EIS datasets concurrently at several targeted SoC levels from 100% to 60%. EIS data is collected using a sinusoidal perturbation signal, which sweeps from 200 kHz to 1 mHz. Raman spectra are collected concurrently at 0, 60, 120, and 180 minutes (200 - 42.7 kHz, 3.86 mHz, 1.78 mHz, and 1.221 mHz, respectively) using a 100 mW 532 nm laser. In Figure 1, the Raman spectra on the left show how the onset of Li₂S₆ correlates with changes in the EIS data. Raman spectra of the first-cycle discharge show an increase in intensity in the peak at ~436 cm⁻¹, consistent with DFT-predicted modes for Li₂S₆, while the intensity of the peak at ~150 cm⁻¹ decreases as elemental sulfur converts into soluble LiPS. Published LiPS standards and Raman modes calculated using density functional theory (DFT) serve as reference points for identifying LiPS. Synchronizing the acquisition of Raman spectra at specific frequencies within the EIS spectrum, performed at several SoC levels, creates a common dataset that enables linking LiPS chemistry, interfacial kinetics, interphase evolution, and charge transport dynamics. EIS spectral analysis generates equivalent circuit models (ECMs) to quantify electrochemical changes in the cell during cycling. The network of parallel combinations of Rp and CPE branches in the ECM was varied from 2 to 6 pairs across SoC levels to minimize the ECM fit error. The evolution of the fitted ECM at the same SoC levels of interest shows increases in charge-transfer resistance and decreases in corner frequencies from the pristine state as the LiPS concentration increases. A stable ohmic resistance, Rs ~325 Ω, observed in the Nyquist plot on the right in Figure 1, indicates that these observed changes in resistance originate from interfacial processes, likely due to the increasing presence of Li 2 S 6 , as identified from the Raman spectra. This method establishes a characterization technique to gain insights into LiPS formation in Li-S batteries. Synchronization of EIS and Raman spectra enables further investigation into the effectiveness of metal-organic frameworks (MOFs) embedded in the cathode and the separator. Beyond Li-S research, this method will be a critical tool for evaluating emerging chemistries and assessing the effectiveness of approaches to improve Coulombic efficiency, reduce capacity fade, increase active material utilization, and limit parasitic side reactions. Figure 1. Raman spectra (left) measured concurrently with electrochemical impedance spectra (right), both collected from an optically accessible Cathode Clarity Li-S CR2023 coin cell. The battery was charged and discharged at a c-rate of 1.4 from a pristine state of charge (SoC) at 100%, down to 60%, and then recharged to 85% SoC. Raman spectra reveal an increasing ~436 cm⁻¹ peak during first-cycle discharge, consistent with Li₂S₆ formation, while the ~150 cm⁻¹ peak decreases as the system consumes elemental sulfur. Figure 1
Zitieren
APA
Reyes, Y. D., Miranda, D., Dirlam, P. T., So, M., & Meehan, K. (2026). In Operando Measurement of Lithium Polysulfide Dynamics in a Modified CR2023 Battery: Synchronized Electrochemical Impedance and Raman Spectroscopy to Monitor Shuttling and Interfacial Kinetics. ECS Meeting Abstracts, MA2026-01(3), 272-272. https://doi.org/10.1149/ma2026-013272mtgabs
Vancouver
Reyes YD, Miranda D, Dirlam PT, So M, Meehan K. In Operando Measurement of Lithium Polysulfide Dynamics in a Modified CR2023 Battery: Synchronized Electrochemical Impedance and Raman Spectroscopy to Monitor Shuttling and Interfacial Kinetics. ECS Meeting Abstracts. 2026;MA2026-01(3):272-272. doi:10.1149/ma2026-013272mtgabs
BibTeX
@article{Reyes2026,
author = {Reyes, Yolanda Denise and Miranda, Daryl and Dirlam, Philip T and So, Monica and Meehan, Kathleen},
title = {In Operando Measurement of Lithium Polysulfide Dynamics in a Modified CR2023 Battery: Synchronized Electrochemical Impedance and Raman Spectroscopy to Monitor Shuttling and Interfacial Kinetics},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {3},
pages = {272--272},
doi = {10.1149/ma2026-013272mtgabs}
}
EUVIMED