Abstract (Originalsprache)
In a rapidly evolving world, there is a growing need for clean and new sustainable energy storage systems. Currently, commercially available Li-ion batteries are the go-to option, but there is room for improvement in their design. One promising way for enhancing silicon-based battery performance is the use of silicon/graphite-composite anodes allowing the mitigation of the drastic volume variations that typically lead to the degradation of the electrode upon cycling. However, the lithiation/delithiation mechanisms, the behavior of stored lithium as well as the SEI (Solid Electrolyte Interphase) formation and evolution involved in this approach have not been extensively studied 1 . To improve interface engineering and gain a deeper understanding of lithium dynamical properties, new characterization approaches are thus necessary. This study aims at achieving this through innovative characterization methods based on 6/7 Li isotope labeling, combining MAS 6/7 Li NMR spectroscopy with mass spectrometry techniques such as ToF-SIMS and FIB-SIMS 2 . In a first step, to trace the movement of lithium in the electrode and SEI it is essential to establish a method to quantify 6 Li and 7 Li isotopes. ssNMR represents an incredible analytical tool for investigating the entire electrode, due to its ability to probe the chemical environments of atomic nuclei. In Li NMR for Si-C/Gr electrodes it is possible to distinguish their lithiation phases as well as SEI. However, the intensity of 7 Li and 6 Li NMR spectra cannot be compared directly for quantification, thus it is mandatory to establish a correct normalization S-factor and use a calibration curve 3 . Then, in a full or half cell the lithium metal electrode and/or the electrolyte have been enriched in 6 Li or 7 Li isotopes to investigate the electrode/electrolyte SEI and the bulk of active material, exploring their evolution upon the ageing/cycling. This methodology enables the tracking of the lithium ions in the various components of the interphase and electrode. Such approach will shed light on Li mobility or trapping in the SEI and at the electrode scale during cycling. In this presentation, we will first introduce the ssNMR-based Li isotope tracing methodology, before discussing our experimental results. Then, we will present possible paths for lithiation of Si and Gr in Si-C/Gr composite electrodes that were observed during the 6/7 Li NMR experiments. Additionally, Li migration from Gr to Si is observed in the composite electrode, as already reported in several articles on Si-Gr composites. Using 6 Li/ 7 Li labelling, normalization S-factor and the deconvolution of NMR spectra, we attempt to trace this complex migration quantitatively and qualitatively 4–6 . (1) Berhaut, C. L.; Dominguez, D. Z.; Tomasi, D.; Vincens, C.; Haon, C.; Reynier, Y.; Porcher, W.; Boudet, N.; Blanc, N.; Chahine, G. A.; Tardif, S.; Pouget, S.; Lyonnard, S. Prelithiation of Silicon/Graphite Composite Anodes: Benefits and Mechanisms for Long-Lasting Li-Ion Batteries. Energy Storage Materials 2020 , 29 , 190–197. https://doi.org/10.1016/j.ensm.2020.04.008. (2) Delfino, P. M.; Bofanova, M.; De Vito, E.; Dupré, N.; Lamblin, G.; Porcher, W.; Wirtz, T.; Audinot, J.-N. Lift-Out Specimen Preparation and Multiscale Correlative Investigation of Li-Ion Battery Electrodes Using Focused Ion Beam-Secondary Ion Mass Spectrometry Platforms. ACS Appl. Mater. Interfaces 2024 , 16 (42), 57141–57150. https://doi.org/10.1021/acsami.4c12915. (3) Berthault, M. Etude de la dynamique du lithium dans un système électrochimique Li-ion par traçage isotopique en combinant les spectrométries RMN et ToF-SIMS. phdthesis, Université Grenoble Alpes [2020-....], 2021. https://theses.hal.science/tel-03274004 (accessed 2023-04-10). (4) Zhang, Y.; Wang, W.; Zhao, Y.; Zhang, X.; Guo, H.; Gao, H.; Xu, D.; Zhao, Y.; Li, G.; Liang, J.; Xin, S.; Guo, Y. Exacerbated High‐Temperature Calendar Aging of SiO x ‐Graphite Electrode Induced by Interparticle Lithium Crosstalk. Adv Funct Materials 2024 , 34 (2), 2310309. https://doi.org/10.1002/adfm.202310309. (5) Berhaut, C. L.; Mirolo, M.; Dominguez, D. Z.; Martens, I.; Pouget, S.; Herlin‐Boime, N.; Chandesris, M.; Tardif, S.; Drnec, J.; Lyonnard, S. Charge Dynamics Induced by Lithiation Heterogeneity in Silicon‐Graphite Composite Anodes. Advanced Energy Materials 2023 , 13 (44), 2301874. https://doi.org/10.1002/aenm.202301874. (6) Moon, J.; Lee, H. C.; Jung, H.; Wakita, S.; Cho, S.; Yoon, J.; Lee, J.; Ueda, A.; Choi, B.; Lee, S.; Ito, K.; Kubo, Y.; Lim, A. C.; Seo, J. G.; Yoo, J.; Lee, S.; Ham, Y.; Baek, W.; Ryu, Y.-G.; Han, I. T. Interplay between Electrochemical Reactions and Mechanical Responses in Silicon–Graphite Anodes and Its Impact on Degradation. Nat Commun 2021 , 12 (1), 2714. https://doi.org/10.1038/s41467-021-22662-7. Figure 1
Zitieren
APA
Dupre, N., Bofanova, M., Delfino, P. M., Audinot, J., Märker, K., Porcher, W., & Vito, E. D. (2026). Exploring Li Pathways in Si-C/Gr SEI Using Li Isotope Tracing. ECS Meeting Abstracts, MA2026-01(3), 236-236. https://doi.org/10.1149/ma2026-013236mtgabs
Vancouver
Dupre N, Bofanova M, Delfino PM, Audinot J, Märker K, Porcher W, et al. Exploring Li Pathways in Si-C/Gr SEI Using Li Isotope Tracing. ECS Meeting Abstracts. 2026;MA2026-01(3):236-236. doi:10.1149/ma2026-013236mtgabs
BibTeX
@article{Dupre2026,
author = {Dupre, Nicolas and Bofanova, Mariia and Delfino, Pablo Maria and Audinot, Jean-Nicolas and Märker, Katharina and Porcher, Willy and Vito, Eric De},
title = {Exploring Li Pathways in Si-C/Gr SEI Using Li Isotope Tracing},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {3},
pages = {236--236},
doi = {10.1149/ma2026-013236mtgabs}
}
EUVIMED