EUVIMEDEUVIMED entdecken
Crossref

Electrochemical and Interfacial Effects of Added Elevated Hydrofluoric Acid Levels in Li-Ion Battery Electrolytes

Shipra Garg, Monica Lee Usrey, Liu Amy Zhou, Brian M Kerber, Tadahiko Kubota

ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (3) · 221-221

DOI: 10.1149/ma2026-013221mtgabs ↗

Kurz gefasst

Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Shipra Garg und 4 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

LiPF 6 is the most widely used salt in commercial lithium-ion batteries because of its high ionic conductivity, its ability to passivate aluminum current collector, and its role in SEI formation on graphite anodes.¹ Despite these advantages, LiPF 6 exhibits poor thermal stability and is highly sensitive to protic impurities such as water, leading to decomposition that can significantly degrade lithium-ion battery performance, particularly under the demanding conditions of modern industrial applications. In the presence of moisture, LiPF 6 decomposition results in the formation of hydrofluoric acid (HF),² which can cause several detrimental effects in lithium-ion cells, including thicker SEI formation, transition metal dissolution and gas generation.³ In this study, we examined the influence of HF concentrations added up to 1000 ppm on multiple cell chemistries (Graphite/NMC811, Graphite/LFP, LTO/LFP) under formation, 45°C cycling, 60°C storage, and 60°C voltage hold conditions. Contrary to expectations, no measurable differences were observed in electrochemical performance metrics across the HF range investigated (added up to 1000 ppm), even under accelerated aging protocols. The absence of observable performance degradation motivated a deeper investigation into the underlying electrochemical and interfacial processes associated with elevated HF levels. To develop mechanistic insight beyond bulk electrochemical behavior, extensive post-test analyses were conducted. Post-test analyses included scanning electron microscopy (SEM) of the anode and cathode and inductively coupled plasma (ICP) of the anode to assess transition metal deposition content. These techniques enabled correlation of electrochemical signatures with chemical and interfacial phenomena occurring during formation and aging. This presentation will combine electrochemical and post-test analyses to explore the impact of HF on electrolyte-electrode interactions. Surprisingly, even at elevated HF concentrations, no significant performance degradation was observed. These unexpected findings offer an opportunity to discuss the underlying mechanisms and explore how such insights inform the design of lithium-ion systems. References: Sascha Nowak and Martin Winter 2015 J. Electrochem. Soc. 162 A2500 Hui Yang et al 2006 J. Power Sources 161 573 Weishan Li 2020 J. Electrochem. Soc. 167 090514

Zitieren

APA

Garg, S., Usrey, M. L., Zhou, L. A., Kerber, B. M., & Kubota, T. (2026). Electrochemical and Interfacial Effects of Added Elevated Hydrofluoric Acid Levels in Li-Ion Battery Electrolytes. ECS Meeting Abstracts, MA2026-01(3), 221-221. https://doi.org/10.1149/ma2026-013221mtgabs

Vancouver

Garg S, Usrey ML, Zhou LA, Kerber BM, Kubota T. Electrochemical and Interfacial Effects of Added Elevated Hydrofluoric Acid Levels in Li-Ion Battery Electrolytes. ECS Meeting Abstracts. 2026;MA2026-01(3):221-221. doi:10.1149/ma2026-013221mtgabs

BibTeX
@article{Garg2026,
  author = {Garg, Shipra and Usrey, Monica Lee and Zhou, Liu Amy and Kerber, Brian M and Kubota, Tadahiko},
  title = {Electrochemical and Interfacial Effects of Added Elevated Hydrofluoric Acid Levels in Li-Ion Battery Electrolytes},
  journal = {ECS Meeting Abstracts},
  year = {2026},
  volume = {MA2026-01},
  number = {3},
  pages = {221--221},
  doi = {10.1149/ma2026-013221mtgabs}
}