On-Board Estimation of Silicon Burn-out in Lithium-Ion Batteries with Silicon-Graphite Composite Anodes

Zhiwen Wan, Andrew Weng, Sravan Pannala, Hamidreza Movahedi, Taylor R. Garrick, Gregory James Offer, Jason Siegel, Anna Stefanopoulou

ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (1) · 91-91

DOI: 10.1149/ma2026-01191mtgabs ↗

Kurz gefasst

Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Zhiwen Wan und 7 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Silicon–graphite (Si/Gr) composite anodes are increasingly adopted to boost cell-level energy density, yet their practical benefit is often curtailed by rapid aging associated with silicon burn-out. Ex-situ studies have clarified key mechanisms, including silicon cracking and repeated SEI re-formation [1]. However, an on-board, in-situ diagnostic capability that can quantify material-specific degradation under real operating constraints remains limited. Methods such as incremental capacity analysis (ICA) and differential voltage analysis (DVA) are easy to deploy, but the overlapping thermodynamic responses of silicon and graphite complicate quantitative attribution of degradation modes to each material [2]. Meanwhile, electrode state-of-health approaches can recover electrode-level properties, but commonly assume fixed electrode open-circuit potentials (OCPs), an assumption that can break down for composite electrodes whose effective OCP evolves with unbalanced material aging [3]. Here we present a physics-informed, BMS-oriented diagnostic framework tailored to Si/Gr anodes that couples (i) the thermodynamic fingerprint of a composite electrode with (ii) silicon-induced kinetic effects that manifest under practical charge/discharge conditions. The algorithm is validated across scales, combining ex-situ material/electrode evidence with in-operando full-cell measurements tracked throughout life [4], demonstrating consistent identification of material-resolved degradation progression. To enable confident deployment in real vehicles, we further quantify estimation uncertainty under non-ideal conditions typical of onboard data: variable sampling rates, changing charge rates relative to laboratory protocols, and partial state-of-charge windows dictated by user behavior. By providing error bounds alongside the inferred material degradation metrics, the framework supports robust interpretation across diverse usage scenarios and enables reliable tracking of silicon and graphite aging contributions. Together, these capabilities provide a practical path toward actionable, quantitative diagnostics and unlock the full potential of high-energy Si/Gr batteries. Figure 1

Zitieren

APA

Wan, Z., Weng, A., Pannala, S., Movahedi, H., Garrick, T. R., Offer, G. J., Siegel, J., & Stefanopoulou, A. (2026). On-Board Estimation of Silicon Burn-out in Lithium-Ion Batteries with Silicon-Graphite Composite Anodes. ECS Meeting Abstracts, MA2026-01(1), 91-91. https://doi.org/10.1149/ma2026-01191mtgabs

Vancouver

Wan Z, Weng A, Pannala S, Movahedi H, Garrick TR, Offer GJ, et al. On-Board Estimation of Silicon Burn-out in Lithium-Ion Batteries with Silicon-Graphite Composite Anodes. ECS Meeting Abstracts. 2026;MA2026-01(1):91-91. doi:10.1149/ma2026-01191mtgabs

BibTeX
@article{Wan2026,
  author = {Wan, Zhiwen and Weng, Andrew and Pannala, Sravan and Movahedi, Hamidreza and Garrick, Taylor R. and Offer, Gregory James and Siegel, Jason and Stefanopoulou, Anna},
  title = {On-Board Estimation of Silicon Burn-out in Lithium-Ion Batteries with Silicon-Graphite Composite Anodes},
  journal = {ECS Meeting Abstracts},
  year = {2026},
  volume = {MA2026-01},
  number = {1},
  pages = {91--91},
  doi = {10.1149/ma2026-01191mtgabs}
}
Kostenlos starten →