Localized Defective Zone Formation Driven by Selective Li + Extraction Defines the High-Voltage Threshold of LiNi 0.6 Co 0.2 Mn 0.2 O 2

Un-Hyuck Kim

ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (11) · 897-897

DOI: 10.1149/ma2026-0111897mtgabs ↗

Kurz gefasst

Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Un-Hyuck Kim.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To clarify the degradation limits of Ni-rich cathodes, we performed a comprehensive analysis of the structural evolution of LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NCM622) under deep delithiation conditions (4.3–4.7 V). Our findings indicate that structural integrity is compromised above 4.5 V, where intragranular fracturing begins to occur alongside intergranular cracking. This mechanical breakdown is attributed to heterogeneous Li + extraction, which induces the formation of alternating defect-rich and defect-free microstructural bands. Notably, we observed the nucleation of cracks at the interfaces of these bands and identified a previously unreported intermediate phase within the defective regions. Electrochemical assessments suggest that 4.5 V represents the critical upper limit for reversible cycling. Consequently, we propose that mitigating surface concentration gradients is essential to suppress localized degradation and unlock the high-voltage potential of NCM622.

Zitieren

APA

Kim, U. (2026). Localized Defective Zone Formation Driven by Selective Li + Extraction Defines the High-Voltage Threshold of LiNi 0.6 Co 0.2 Mn 0.2 O 2. ECS Meeting Abstracts, MA2026-01(11), 897-897. https://doi.org/10.1149/ma2026-0111897mtgabs

Vancouver

Kim U. Localized Defective Zone Formation Driven by Selective Li + Extraction Defines the High-Voltage Threshold of LiNi 0.6 Co 0.2 Mn 0.2 O 2. ECS Meeting Abstracts. 2026;MA2026-01(11):897-897. doi:10.1149/ma2026-0111897mtgabs

BibTeX
@article{Kim2026,
  author = {Kim, Un-Hyuck},
  title = {Localized Defective Zone Formation Driven by Selective Li + Extraction Defines the High-Voltage Threshold of LiNi 0.6 Co 0.2 Mn 0.2 O 2},
  journal = {ECS Meeting Abstracts},
  year = {2026},
  volume = {MA2026-01},
  number = {11},
  pages = {897--897},
  doi = {10.1149/ma2026-0111897mtgabs}
}
Kostenlos starten →