Mechanism of Internal Short Circuits in Lithium-Ion Batteries Under Mechanical Abuse
ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (1) · 117-117
DOI: 10.1149/ma2026-011117mtgabs ↗Kurz gefasst
Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Shuguo Sun und 2 weiteren Autor:innen.
Abstract (Originalsprache)
Internal short circuits (ISCs) in lithium-ion batteries (LIBs) arising from mechanical failure of separators represent a critical early-stage safety event. This study investigates the initiation and evolution of ISCs under mechanical abusive loading using ball indentation of electrode stacks, with a focus on resolving the layer-by-layer failure behavior within a representative anode–separator–cathode unit. Here, we introduce a Unit-Resolved Detection (URD) methodology that enables in situ electrochemo-mechanical monitoring of individual cathode-separator-anode units under controlled mechanical abuse. Using this approach, we examine the effects of boundary conditions, state of charge (SOC), and strain rate to elucidate the underlying mechanisms that trigger ISC formation. Our results reveal that ISC initiation occurs sequentially from layer to layer. Under a hard bottom boundary, the top anode-separator-cathode unit fails first, and ISC propagation follows a top-to-bottom sequence. In contrast, under soft boundary constraints, the triggering order reverses entirely, reflecting the redistribution of local strain imposed by the boundary condition. A detailed mechanics-based multilayer model incorporating multiple anode–separator–cathode units and anisotropic material properties accurately captures these measured responses and reproduces both component-level and stack-level mechanical behavior. Systematic analysis of the coupled electrochemical, mechanical, and thermal responses demonstrates how boundary conditions, separator defects, and strain rate govern ISC onset and progression. Two distinct ISC modes, i.e. , soft (S-ISC) and hard (H-ISC), are from voltage evolution signatures and post-mortem forensic evidence. To further classify failure states, we propose a dimensionless electrochemo-mechanical sensitivity index (ESI) that quantifies the interaction among mechanical deformation, electrochemical conditions, and ISC severity. In addition, higher strain rates accelerate separator failure, leading to earlier ISC initiation at smaller applied strains. Elevated loading rates triggered ISCs up to 18% earlier than quasi-static loading, consistent with the reduced failure strain of separators under dynamic conditions. Numerical simulations reproduce these trends, confirming that strain-rate-dependent mechanical weakening of the separator is the primary mechanism driving earlier ISC onset at rapid loading speeds. Overall, the URD framework provides a quantitative link between mechanical deformation and electrochemical failure. This approach offers a powerful platform for designing mechanically robust and intrinsically safer lithium-ion batteries for electric vehicles and grid-scale energy storage systems.
Zitieren
APA
Sun, S., Rui, B., & Xu, J. (2026). Mechanism of Internal Short Circuits in Lithium-Ion Batteries Under Mechanical Abuse. ECS Meeting Abstracts, MA2026-01(1), 117-117. https://doi.org/10.1149/ma2026-011117mtgabs
Vancouver
Sun S, Rui B, Xu J. Mechanism of Internal Short Circuits in Lithium-Ion Batteries Under Mechanical Abuse. ECS Meeting Abstracts. 2026;MA2026-01(1):117-117. doi:10.1149/ma2026-011117mtgabs
BibTeX
@article{Sun2026,
author = {Sun, Shuguo and Rui, Bo and Xu, Jun},
title = {Mechanism of Internal Short Circuits in Lithium-Ion Batteries Under Mechanical Abuse},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {1},
pages = {117--117},
doi = {10.1149/ma2026-011117mtgabs}
}
EUVIMED