Synergistic Degradation of 18650-Type NCA Cells Under Overcharge–Thermal Coupled Stress
ECS Meeting Abstracts · 07.07.2026 · MA2026-01 (1) · 101-101
DOI: 10.1149/ma2026-011101mtgabs ↗Kurz gefasst
Fachartikel in der Zeitschrift ECS Meeting Abstracts, erschienen am 07.07.2026. Verfasst von Minje Kim und 4 weiteren Autor:innen.
Abstract (Originalsprache)
With the rapid expansion of electric vehicles, ensuring the safety of high-energy-density lithium-ion batteries has become increasingly critical. Ternary cathodes such as LiNi x Co y Al 1-x-y O 2 (NCA) are widely adopted due to their high energy density; however, their thermal and electrochemical stability deteriorate significantly under overcharge and elevated-temperature conditions. Although previous studies have investigated battery degradation using electrochemical diagnostic techniques, most have focused on isolated stressors or low-rate, constant-temperature conditions, providing limited insight into degradation mechanisms under realistic, coupled abuse scenarios. In this study, we systematically investigate the degradation behavior of 18650-type NCA lithium-ion cells subjected to 3C overcharge at elevated temperatures ranging from 30 to 50 °C. Incremental capacity analysis (ICA) and electrochemical impedance spectroscopy (EIS) reveal distinct temperature-dependent degradation pathways: at 30 °C, gradual attenuation of the Ni 4+ /Ni 3+ reduction peak near 4.1 V indicates progressive loss of electrochemical reversibility, whereas at 50 °C a new reduction feature around 3.1 V emerges, suggesting delayed lithium-ion transport and abrupt interfacial deterioration. These electrochemical signatures correlate with increased interfacial resistance and are further supported by material analysis, confirming lattice collapse, carbon structure collapse, and heterogeneous growth of the cathode–electrolyte interphase (CEI). Notably, elevated temperatures induce the formation of a thicker yet structurally discontinuous CEI, while lower temperatures result in thinner but more gradually degraded interphases. Gas evolution measurements further reveal contrasting behaviors, with sharp CO 2 release at 30 °C beyond a critical degradation point and suppressed gas evolution at 50 °C, likely due to the thickened CEI. These results highlight the synergistic nature of degradation under concurrent overcharge and thermal stress, offering new insights into degradation mechanisms of ternary cathode lithium-ion batteries under realistic abuse conditions.
Zitieren
APA
Kim, M., Jung, J., Kim, M., Song, S., & Nah, J. (2026). Synergistic Degradation of 18650-Type NCA Cells Under Overcharge–Thermal Coupled Stress. ECS Meeting Abstracts, MA2026-01(1), 101-101. https://doi.org/10.1149/ma2026-011101mtgabs
Vancouver
Kim M, Jung J, Kim M, Song S, Nah J. Synergistic Degradation of 18650-Type NCA Cells Under Overcharge–Thermal Coupled Stress. ECS Meeting Abstracts. 2026;MA2026-01(1):101-101. doi:10.1149/ma2026-011101mtgabs
BibTeX
@article{Kim2026,
author = {Kim, Minje and Jung, Jonghyuk and Kim, Minji and Song, Suchan and Nah, Junghyo},
title = {Synergistic Degradation of 18650-Type NCA Cells Under Overcharge–Thermal Coupled Stress},
journal = {ECS Meeting Abstracts},
year = {2026},
volume = {MA2026-01},
number = {1},
pages = {101--101},
doi = {10.1149/ma2026-011101mtgabs}
}
EUVIMED