Effects of Si Poisoning on Microstructure of Ni-Cermet Fuel Electrodes During Solid Oxide Electrolysis Cell Durability Test

Kei Yamada, Kazutaka Ikegawa, Kyoko Matsubara, Yoshihisa Yamamoto, Yuya Tachikawa, Junko Matsuda, Kazunari Sasaki

Journal of The Electrochemical Society · 12.06.2026 · 173 (11) · 114502

DOI: 10.1149/1945-7111/ae720c ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of The Electrochemical Society, online erschienen am 02.06.2026. Verfasst von Kei Yamada und 6 weiteren Autor:innen. Die Arbeit nennt 48 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Japan Science and Technology Agency, New Energy and Industrial Technology Development Organization.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The primary factors contributing to the performance degradation of SOEC fuel electrodes are the aggregation and migration of nickel (Ni) catalysts, as well as the influence of impurities in the fuel gas. In this study, to investigate the degradation phenomena and their underlying causes associated with differences in the oxides of Ni-cermet fuel electrodes, three types of fuel electrodes, namely, Ni-scandia-stabilized zirconia (ScSZ) cermet and two types of Ni-gadolinium-doped ceria (GDC) cermets, were subjected to SOEC durability tests at 800 °C for 1000 h using 50% humidified hydrogen as fuel, with a current density of −0.2 A cm −2 . SEM and STEM observations of cross-sections of each fuel electrode before and after the 1000 h test revealed differences in the precipitation behavior of silica components in the Ni-ScSZ and Ni-GDC fuel electrodes: in the Ni-ScSZ, SiO 2 was primarily precipitated at the electrode/electrolyte interface, whereas Ce-Si-O with the same crystal structure as Ce 2 Si 2 O 7 was precipitated from the fuel electrode surface (Pt mesh side) in the Ni-GDC system, covering the Ni and GDC particle surfaces in the fuel electrode. During the initial stage of long-term SOEC operation, the formation of Ce-Si-O does not significantly affect the electrode activity while the electrode/electrolyte interface remains intact. However, when the Ce-Si-O reaction phase spreads across the entire electrodes, the degradation of the electrode activity may accelerate via other mechanisms, such as Ni oxidation and aggregation.

Förderung

  • Japan Science and Technology Agency
  • New Energy and Industrial Technology Development Organization

Zitieren

APA

Yamada, K., Ikegawa, K., Matsubara, K., Yamamoto, Y., Tachikawa, Y., Matsuda, J., & Sasaki, K. (2026). Effects of Si Poisoning on Microstructure of Ni-Cermet Fuel Electrodes During Solid Oxide Electrolysis Cell Durability Test. Journal of The Electrochemical Society, 173(11), 114502. https://doi.org/10.1149/1945-7111/ae720c

Vancouver

Yamada K, Ikegawa K, Matsubara K, Yamamoto Y, Tachikawa Y, Matsuda J, et al. Effects of Si Poisoning on Microstructure of Ni-Cermet Fuel Electrodes During Solid Oxide Electrolysis Cell Durability Test. Journal of The Electrochemical Society. 2026;173(11):114502. doi:10.1149/1945-7111/ae720c

BibTeX
@article{Yamada2026,
  author = {Yamada, Kei and Ikegawa, Kazutaka and Matsubara, Kyoko and Yamamoto, Yoshihisa and Tachikawa, Yuya and Matsuda, Junko and Sasaki, Kazunari},
  title = {Effects of Si Poisoning on Microstructure of Ni-Cermet Fuel Electrodes During Solid Oxide Electrolysis Cell Durability Test},
  journal = {Journal of The Electrochemical Society},
  year = {2026},
  volume = {173},
  number = {11},
  pages = {114502},
  doi = {10.1149/1945-7111/ae720c}
}
Kostenlos starten →