The Origin of High Voltage Degradation in O3-Layered Oxide/Hard Carbon Sodium-Ion Pouch Cells

Ziwei Ye, Libin Zhang, Hussein Hijazi, Ben Tang, Yixiang Zhang, Svena Yu, Haoqi Ni, Bailey Rutherford, J. R. Dahn, Michael Metzger

Journal of The Electrochemical Society · 14.01.2026 · 173 (1) · 010506

DOI: 10.1149/1945-7111/ae2f2e ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of The Electrochemical Society, online erschienen am 08.01.2026. Verfasst von Ziwei Ye und 9 weiteren Autor:innen. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The O3-type sodium layered oxide NaMO 2 , where M is a mix of Mn, Fe, Ni and Zn, here NaMn 0.39 Fe 0.31 Ni 0.22 Zn 0.08 O 2 , has a specific capacity of ∼140 mAh g −1 when charged to 4.0 V, highlighting its potential as a positive electrode material for sodium-ion batteries. Electrochemical tests on machine-made pouch cells indicate that increasing the upper cut-off voltage from 3.8 to 3.9 V and 4.0 V leads to initially higher capacity which fades rapidly over cycling. Isothermal microcalorimetry, ultra-high precision coulometry and micro-X-ray fluorescence spectroscopy ruled out parasitic reactions between the electrolyte and the partially de-sodiated positive electrode surface as a major contributing factor to the inferior electrochemical performance at 4.0 V. Instead, it was found by ex situ and in situ X-ray diffraction that repeated cycling to 4.0 V induces the formation of an octahedral/prismatic hybrid phase, which leads to a collapse of the c lattice parameter in the crystal structure, resulting in poor long-term reversibility and ultimately poor cycle life. This irreversible structure transformation is the primary mechanism for poor cycling stability of the O3-type sodium layered oxide NaMO 2 at high voltage.

Zitieren

APA

Ye, Z., Zhang, L., Hijazi, H., Tang, B., Zhang, Y., Yu, S., Ni, H., Rutherford, B., Dahn, J. R., & Metzger, M. (2026). The Origin of High Voltage Degradation in O3-Layered Oxide/Hard Carbon Sodium-Ion Pouch Cells. Journal of The Electrochemical Society, 173(1), 010506. https://doi.org/10.1149/1945-7111/ae2f2e

Vancouver

Ye Z, Zhang L, Hijazi H, Tang B, Zhang Y, Yu S, et al. The Origin of High Voltage Degradation in O3-Layered Oxide/Hard Carbon Sodium-Ion Pouch Cells. Journal of The Electrochemical Society. 2026;173(1):010506. doi:10.1149/1945-7111/ae2f2e

BibTeX
@article{Ye2026,
  author = {Ye, Ziwei and Zhang, Libin and Hijazi, Hussein and Tang, Ben and Zhang, Yixiang and Yu, Svena and Ni, Haoqi and Rutherford, Bailey and Dahn, J. R. and Metzger, Michael},
  title = {The Origin of High Voltage Degradation in O3-Layered Oxide/Hard Carbon Sodium-Ion Pouch Cells},
  journal = {Journal of The Electrochemical Society},
  year = {2026},
  volume = {173},
  number = {1},
  pages = {010506},
  doi = {10.1149/1945-7111/ae2f2e}
}
Kostenlos starten →