Characterization of Cycle-Aged Commercial NMC and NCA Lithium-ion Cells: I. Temperature-Dependent Degradation

Reed Wittman, Matthieu Dubarry, Sergei Ivanov, Benjamin W. Juba, Jessica Romàn-Kustas, Armando Fresquez, Jill Langendorf, Richard Grant, Gretchen Taggart, Babu Chalamala, Yuliya Preger

Journal of The Electrochemical Society · 01.12.2023 · 170 (12) · 120538

DOI: 10.1149/1945-7111/ad1450 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of The Electrochemical Society, online erschienen am 28.12.2023. Verfasst von Reed Wittman und 10 weiteren Autor:innen. Die Arbeit wurde bisher 32-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Office of Electricity Delivery and Energy Reliability.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Lithium-ion batteries are widely used in applications from consumer electronic devices to stationary energy storage. Appropriate management of batteries is challenging due to limited data on their performance and materials degradation. Previous studies have focused on characterization of single cells under specific operating conditions. In the present work, commercial 18650 lithium-ion cells with LiNi x Mn y Co 1-x-y O 2 (NMC) and LiNi x Co y Al 1-x-y O 2 (NCA) positive electrodes were characterized by a wide range of electrochemical and materials techniques after cycling at 15, 25, or 35 °C to ∼80% capacity. The NCA cells exhibit weak temperature dependence in their cycle aging and materials degradation. The NMC cells exhibited increased capacity fade and materials degradation as ambient temperature decreased. All cells exhibited loss of lithium inventory as their primary degradation mode. However, the NCA cells only showed evidence of solid electrolyte interphase (SEI) growth whereas the NMC cells showed signs of Li plating at 15 °C, transitioning to SEI growth at 35 °C. The NMC cells displayed signs of loss of active material at the positive electrode at lower temperatures, suggesting that Li plating is correlated to additional processes that increase the rate of degradation. These results highlight the importance of avoiding broad generalizations about Li-ion battery temperature dependence.

Förderung

  • Office of Electricity Delivery and Energy Reliability

Zitieren

APA

Wittman, R., Dubarry, M., Ivanov, S., Juba, B. W., Romàn-Kustas, J., Fresquez, A., Langendorf, J., Grant, R., Taggart, G., Chalamala, B., & Preger, Y. (2023). Characterization of Cycle-Aged Commercial NMC and NCA Lithium-ion Cells: I. Temperature-Dependent Degradation. Journal of The Electrochemical Society, 170(12), 120538. https://doi.org/10.1149/1945-7111/ad1450

Vancouver

Wittman R, Dubarry M, Ivanov S, Juba BW, Romàn-Kustas J, Fresquez A, et al. Characterization of Cycle-Aged Commercial NMC and NCA Lithium-ion Cells: I. Temperature-Dependent Degradation. Journal of The Electrochemical Society. 2023;170(12):120538. doi:10.1149/1945-7111/ad1450

BibTeX
@article{Wittman2023,
  author = {Wittman, Reed and Dubarry, Matthieu and Ivanov, Sergei and Juba, Benjamin W. and Romàn-Kustas, Jessica and Fresquez, Armando and Langendorf, Jill and Grant, Richard and Taggart, Gretchen and Chalamala, Babu and Preger, Yuliya},
  title = {Characterization of Cycle-Aged Commercial NMC and NCA Lithium-ion Cells: I. Temperature-Dependent Degradation},
  journal = {Journal of The Electrochemical Society},
  year = {2023},
  volume = {170},
  number = {12},
  pages = {120538},
  doi = {10.1149/1945-7111/ad1450}
}
Kostenlos starten →