EUVIMEDEUVIMED entdecken
Open Access · CC BY 4.0

Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling

Puvikkarasan Jayapragasam, Yeting Wen, Korey Cook, Jacob A. Wrubel, Zhiwen Ma, Kevin Huang, Xinfang Jin

Journal of The Electrochemical Society · 01.05.2023 · 170 (5) · 054509

DOI: 10.1149/1945-7111/acd4f1 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of The Electrochemical Society, online erschienen am 23.05.2023. Verfasst von Puvikkarasan Jayapragasam und 6 weiteren Autor:innen. Die Arbeit wurde bisher 14-mal zitiert (Crossref) und nennt 43 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: U.S. Department of Energy's Office of Energy Efficiency and Renewable Energy.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Solid oxide electrolysis cell (SOEC) is a very efficient hydrogen production technology, but the cell degradation is a serious limiting factor for its long-term implementation. Oxygen electrode (OE) delamination is reported to be the critical degradation mechanism. In this study, we present a methodology to understand the delamination failure of the OE due to chemical stress in a better perspective. Several OE configurations were tested: baseline strontium-doped lanthanum cobalt iron oxide (LSCF) single layer design and tantalum-doped strontium cobalt oxide (SCT) - LSCF bilayer designs with different SCT loadings. An electro-chemo-mechanical model is developed to associate the electrochemical behavior of the cell with solid mechanics for calculating crack growth of the cell during long term test. The bilayer configuration with SCT 20 wt% has better performance as it survived in the long-term life test with the least crack length. This study implies that an additional nano-coating of SCT over the OE have improved the species transport and oxygen evolution with reduced chemical stress. As the operating current density decreases, it takes longer time for the cell to reach the delamination with the same critical crack length of 6.5 μ m (∼93% of the electrode/electrolyte interface length). Finally, it was concluded that chemical stress plays a significant role in interface delamination failure, however it may not be the only source of stresses at the interface.

Förderung

  • U.S. Department of Energy's Office of Energy Efficiency and Renewable Energy

Zitieren

APA

Jayapragasam, P., Wen, Y., Cook, K., Wrubel, J. A., Ma, Z., Huang, K., & Jin, X. (2023). Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling. Journal of The Electrochemical Society, 170(5), 054509. https://doi.org/10.1149/1945-7111/acd4f1

Vancouver

Jayapragasam P, Wen Y, Cook K, Wrubel JA, Ma Z, Huang K, et al. Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling. Journal of The Electrochemical Society. 2023;170(5):054509. doi:10.1149/1945-7111/acd4f1

BibTeX
@article{Jayapragasam2023,
  author = {Jayapragasam, Puvikkarasan and Wen, Yeting and Cook, Korey and Wrubel, Jacob A. and Ma, Zhiwen and Huang, Kevin and Jin, Xinfang},
  title = {Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling},
  journal = {Journal of The Electrochemical Society},
  year = {2023},
  volume = {170},
  number = {5},
  pages = {054509},
  doi = {10.1149/1945-7111/acd4f1}
}
Kostenlos starten →