Solid-state reaction assisted by sand milling for the preparation of BaTiO 3 powders

Guoyang Zhang, Pengrong Ren, Jiajun Yang, Dong Li, Xin Wang

Journal of Advanced Dielectrics · 29.07.2026

DOI: 10.1142/s2010135x26500256 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Advanced Dielectrics, online erschienen am 29.07.2026. Verfasst von Guoyang Zhang und 4 weiteren Autor:innen. Die Arbeit nennt 25 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Key Research and Development Program of Shaanxi.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

To address the need for synergistic control over both particle size and tetragonal-to-cubic ratio ([Formula: see text] of nano-barium titanate (BaTiO 3 ) powder in multilayer ceramic capacitors (MLCCs), this study employed a solid-phase reaction-assisted sand milling process to systematically investigate the effects of milling medium polarity, mechanical force application during milling, and calcination history on precursor dispersion, stoichiometric ratios, crystal phase evolution, and grain growth behavior. It is demonstrated that using deionized water as the milling medium leverages its high polarity and interfacial compatibility with hydrophilic particle surfaces to effectively suppress BaCO 3 /TiO 2 agglomeration and element segregation, optimizing the Ba/Ti molar ratio to 1.0019. By optimizing milling parameters (2500[Formula: see text]rpm, 10 h), the average particle size reduces to 68.74[Formula: see text]nm, the size distribution narrows to 40−90[Formula: see text]nm, the specific surface area significantly increases, and the solid-phase reaction temperature decreases from the conventional range above 1100 ∘ C to 800–900 ∘ C. Calcination temperature critically governs the synergistic evolution of cubic-to-tetragonal phase transformation and grain growth: at 800–900 ∘ C, the powder maintains a cubic phase ([Formula: see text] 1.000) with grain sizes of 87–109[Formula: see text]nm; beyond 950 ∘ C, grains exceeds the critical size of approximately 156.59[Formula: see text]nm, tetragonal distortion emerges, and the [Formula: see text] ratio monotonically increases from 1.00462 to 1.00881 with rising temperature (up to 1100 ∘ C). The resulting powder exhibits a piezoelectric coefficient ([Formula: see text]) of 219[Formula: see text]pC/N, a mechanical quality factor (Q) ranging from 236 to 269, a planar electromechanical coupling coefficient (k) of 43.2%, a dielectric constant ([Formula: see text]) increasing from 1820 to 2374, and dielectric loss (tan[Formula: see text]) being below 0.025. This study determines the critical grain size for the cubic-to-tetragonal phase transition, achieving precise control over both the particle size and tetragonal structure of nano-BaTiO 3 powder, thereby providing a fundamental process basis for cost-effective and reproducible preparation of dielectric powders for high-end multilayer ceramic capacitors (MLCCs).

Förderung

  • National Natural Science Foundation of China
  • Key Research and Development Program of Shaanxi

Zitieren

APA

Zhang, G., Ren, P., Yang, J., Li, D., & Wang, X. (2026). Solid-state reaction assisted by sand milling for the preparation of BaTiO 3 powders. Journal of Advanced Dielectrics. https://doi.org/10.1142/s2010135x26500256

Vancouver

Zhang G, Ren P, Yang J, Li D, Wang X. Solid-state reaction assisted by sand milling for the preparation of BaTiO 3 powders. Journal of Advanced Dielectrics. 2026. doi:10.1142/s2010135x26500256

BibTeX
@article{Zhang2026,
  author = {Zhang, Guoyang and Ren, Pengrong and Yang, Jiajun and Li, Dong and Wang, Xin},
  title = {Solid-state reaction assisted by sand milling for the preparation of BaTiO 3 powders},
  journal = {Journal of Advanced Dielectrics},
  year = {2026},
  doi = {10.1142/s2010135x26500256}
}
Kostenlos starten →