EUVIMEDEUVIMED entdecken
Crossref

Optimization of thermoelectric power factor in BiSnSe thin films through post-selenization treatment

Wafa Mohammed Almalki, Elsammani Ali Shokralla, Mohamed A. Siddig, Mohamed Abdelsabour Fahmy, Jack Arayro, Lamiaa G. Alharbe, Hind Alqurashi, Arslan Ashfaq

International Journal of Modern Physics B · 20.06.2026 · 40 (15)

DOI: 10.1142/s0217979226501420 ↗

Kurz gefasst

Fachartikel in der Zeitschrift International Journal of Modern Physics B, online erschienen am 06.05.2026. Verfasst von Wafa Mohammed Almalki und 7 weiteren Autor:innen. Die Arbeit nennt 23 Literaturangaben.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, we have synthesized structural and thermoelectric characterization of BiSnSe thin films to post-selenization treatments of varying durations (30, 60, 90, 120 and 150[Formula: see text]min). X-ray diffraction analysis revealed that grown films crystallize in the BiSnSe phase. Post-selenization enhances the crystallinity, reduces micro-strain and increases crystallite size, with the 120[Formula: see text]min treated film achieving the largest crystallites (44[Formula: see text]nm) and lowest micro-strain ([Formula: see text]). Scanning electron microscopy confirms grain growth and improved surface uniformity with selenization, reducing defects and voids. Hall effect measurements show that post-selenization increases the charge carrier concentration from 1.8 [Formula: see text] 10[Formula: see text][Formula: see text]cm[Formula: see text] (as-grown) to 5.1 [Formula: see text] 10[Formula: see text][Formula: see text]cm[Formula: see text] and enhances mobility from 20[Formula: see text]cm 2 V[Formula: see text]s[Formula: see text] to 36[Formula: see text]cm 2 V[Formula: see text]s[Formula: see text] (120[Formula: see text]min). Consequently, the electrical conductivity and Seebeck coefficient are significantly improved, reaching 118[Formula: see text]Scm[Formula: see text] and 246 [Formula: see text]V/K at 550[Formula: see text]K, respectively, for the 120 min film. The corresponding thermoelectric power factor achieves a maximum of 5.38 [Formula: see text]Wcm[Formula: see text]K[Formula: see text], highlighting the optimal selenization duration. The study demonstrates that post-selenization effectively optimizes structural, morphological and electronic properties, providing a viable route for enhancing the thermoelectric performance of BiSnSe thin films.

Zitieren

APA

Almalki, W. M., Shokralla, E. A., Siddig, M. A., Fahmy, M. A., Arayro, J., Alharbe, L. G., Alqurashi, H., & Ashfaq, A. (2026). Optimization of thermoelectric power factor in BiSnSe thin films through post-selenization treatment. International Journal of Modern Physics B, 40(15). https://doi.org/10.1142/s0217979226501420

Vancouver

Almalki WM, Shokralla EA, Siddig MA, Fahmy MA, Arayro J, Alharbe LG, et al. Optimization of thermoelectric power factor in BiSnSe thin films through post-selenization treatment. International Journal of Modern Physics B. 2026;40(15). doi:10.1142/s0217979226501420

BibTeX
@article{Almalki2026,
  author = {Almalki, Wafa Mohammed and Shokralla, Elsammani Ali and Siddig, Mohamed A. and Fahmy, Mohamed Abdelsabour and Arayro, Jack and Alharbe, Lamiaa G. and Alqurashi, Hind and Ashfaq, Arslan},
  title = {Optimization of thermoelectric power factor in BiSnSe thin films through post-selenization treatment},
  journal = {International Journal of Modern Physics B},
  year = {2026},
  volume = {40},
  number = {15},
  doi = {10.1142/s0217979226501420}
}
Kostenlos starten →