Mapping the failure envelope of a filled silicone elastomer to determine a failure criterion
Journal of Rheology · 01.09.2026 · 70 (5) · 1181-1190
DOI: 10.1122/8.0001209 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Rheology, online erschienen am 01.09.2026. Verfasst von Majed N. Saadawi und 1 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 53 Literaturangaben. Gefördert von: University of Akron.
Abstract (Originalsprache)
Multiaxial stress states often develop in common structures, such as joints, corners, and thin-walled shells. Developing criteria that map the failure of materials under multiaxial stress states is thus essential to selecting materials during the design process. Here, failure refers to the catastrophic rupture that occurs in a material upon the development of a critical stress that defines its ultimate strength. While such analyses have long been applied to quantify the yielding behavior of stiff materials, such as metals and glassy polymers, limited measurements of the multiaxial strengths of soft rubbery polymer networks are available in the literature. Using biaxial deformations, this work characterizes the strengths of a commercially available filled silicone elastomer under multiple stress states and maps its failure envelope in planar principal stress space. The first quadrant of planar principal stress space is characterized by applying biaxial extension to cruciform samples. The second quadrant is then mapped by applying both tension and torsion to cylindrical samples. By combining these measurements, it is observed that the failure envelope for this commercially available filled silicone elastomer is consistent with a maximum principal stress failure criterion.
Förderung
- University of Akron
Zitieren
APA
Saadawi, M. N., & Barney, C. W. (2026). Mapping the failure envelope of a filled silicone elastomer to determine a failure criterion. Journal of Rheology, 70(5), 1181-1190. https://doi.org/10.1122/8.0001209
Vancouver
Saadawi MN, Barney CW. Mapping the failure envelope of a filled silicone elastomer to determine a failure criterion. Journal of Rheology. 2026;70(5):1181-1190. doi:10.1122/8.0001209
BibTeX
@article{Saadawi2026,
author = {Saadawi, Majed N. and Barney, Christopher W.},
title = {Mapping the failure envelope of a filled silicone elastomer to determine a failure criterion},
journal = {Journal of Rheology},
year = {2026},
volume = {70},
number = {5},
pages = {1181--1190},
doi = {10.1122/8.0001209}
}
EUVIMED