Influence of Sb content on carrier transport and thermoelectric properties of flexible Bi–Sb films

Zhihao Ben, Guihong Song, Yu Chen, Yusheng Wu, Junhua You

Journal of Vacuum Science & Technology A · 01.01.2025 · 43 (1)

DOI: 10.1116/6.0004097 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Vacuum Science & Technology A, online erschienen am 24.12.2024. Verfasst von Zhihao Ben und 4 weiteren Autor:innen. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 25 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Liaoning Revitalization Talents Program, Liaoning Applied Basic Research Program.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

In this study, the Bi–Sb films with different Sb content on silicon and polyimide (PI) substrates were successfully fabricated via high vacuum magnetron sputtering and the carrier transport and thermoelectric properties were studied. As the Sb content increased, the carrier concentration, electrical conductivity, Seebeck coefficient, and power factor of deposited Bi–Sb films initially increased and then decreased at room temperature. The maximum Seebeck coefficient and power factor reached −108.90 μV K−1 and 0.133mW m−1 K−2 for the Bi84Sb16 film at room temperature. The electrical conductivity, Seebeck coefficient, and power factor of deposited Bi–Sb films increased with increasing energy gap. Whether bending toward or bending back toward, the relative electrical conductivity of the films decreased with increasing bending angle. When the bending angle was less than 90°, the electrical conductivity of the films decreased very little. However, the electrical conductivity of the films exhibited an obvious reduction when the bending angle exceeded 90°. The relative electrical conductivity of the deposited films under bending toward and bending back toward decreased by 4% and 8% under 180° bending angle, respectively. Compared with bending toward, the electrical conductivity of the films bending back toward (tensile) decreases even more at the same bending angle. The electrical conductivity of the films bending toward changed little and remained 94.1% after bending 1000 times at the radius of 3 mm. The maximum power density of a flexible thermoelectric generator for Bi84Sb16 film was 0.672 and 0.8644 W m−2 at ΔT = 30 and 39 K, respectively.

Förderung

  • National Natural Science Foundation of China
  • Liaoning Revitalization Talents Program
  • Liaoning Applied Basic Research Program
  • Shenyang Science and Technology Project

Zitieren

APA

Ben, Z., Song, G., Chen, Y., Wu, Y., & You, J. (2025). Influence of Sb content on carrier transport and thermoelectric properties of flexible Bi–Sb films. Journal of Vacuum Science & Technology A, 43(1). https://doi.org/10.1116/6.0004097

Vancouver

Ben Z, Song G, Chen Y, Wu Y, You J. Influence of Sb content on carrier transport and thermoelectric properties of flexible Bi–Sb films. Journal of Vacuum Science & Technology A. 2025;43(1). doi:10.1116/6.0004097

BibTeX
@article{Ben2025,
  author = {Ben, Zhihao and Song, Guihong and Chen, Yu and Wu, Yusheng and You, Junhua},
  title = {Influence of Sb content on carrier transport and thermoelectric properties of flexible Bi–Sb films},
  journal = {Journal of Vacuum Science & Technology A},
  year = {2025},
  volume = {43},
  number = {1},
  doi = {10.1116/6.0004097}
}
Kostenlos starten →