Fachartikel in der Zeitschrift Journal of Vacuum Science & Technology A, online erschienen am 03.01.2023. Verfasst von Michael E. Liao und 4 weiteren Autor:innen. Die Arbeit wurde bisher 30-mal zitiert (Crossref) und nennt 42 Literaturangaben. Gefördert von: Office of Naval Research.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Smooth (< 0.5 nm rms) and subsurface damage-free (010) β-Ga2O3 was achieved with low-pressure chemical mechanical polishing. An applied pressure of 1 kPa along with colloidal silica and poromeric polyurethane polishing pads rotating at 30 rpm was found to be the optimal polishing parameters for (010) β-Ga2O3. Using higher pressures typically employed in the current literature induced subsurface damage in the substrates. Diffuse scatter intensity of triple-axis x-ray rocking curves was used to determine the presence of subsurface lattice damage, which was quantified by measuring peak widths below the half maximum (i.e., FWXM where X < 0.5). The initially rough surfaces of (010) β-Ga2O3 substrates due to wafer slicing and grinding were lapped and polished. A 5 μm Al2O3 slurry followed by a 0.3 μm Al2O3 slurry was used as the primary lap material removal step. The material removal rates were ∼20 and ∼9 μm/h, respectively. Then, chemical mechanical polishing was performed using colloidal alumina followed by colloidal silica. The removal rates were ∼1.3 and ∼0.4 μm/h, respectively. Only colloidal silica showed the complete removal of subsurface damage. The final (020) β-Ga2O3 rocking curve FWHM was ∼13″ and FW(0.001)M was ∼120″, which matches the widths of commercially available pristine (010) β-Ga2O3. A final cleaning step using dilute bleach and dilute citric acid to remove residual silica slurry particles from the surface was demonstrated.

Förderung

  • Office of Naval Research

Zitieren

APA

Liao, M. E., Huynh, K., Matto, L., Luccioni, D. P., & Goorsky, M. S. (2023). Optimization of chemical mechanical polishing of (010) β-Ga2O3. Journal of Vacuum Science & Technology A, 41(1). https://doi.org/10.1116/6.0002241

Vancouver

Liao ME, Huynh K, Matto L, Luccioni DP, Goorsky MS. Optimization of chemical mechanical polishing of (010) β-Ga2O3. Journal of Vacuum Science & Technology A. 2023;41(1). doi:10.1116/6.0002241

BibTeX
@article{Liao2023,
  author = {Liao, Michael E. and Huynh, Kenny and Matto, Lezli and Luccioni, Dorian P. and Goorsky, Mark S.},
  title = {Optimization of chemical mechanical polishing of (010) β-Ga2O3},
  journal = {Journal of Vacuum Science & Technology A},
  year = {2023},
  volume = {41},
  number = {1},
  doi = {10.1116/6.0002241}
}
Kostenlos starten →