Fachartikel in der Zeitschrift Journal of Prosthodontics, online erschienen am 07.07.2026. Verfasst von Waleed Ahmed Abdelnaby und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Prosthodontics, Faculty of Oral and Dental Medicine, Delta University for Science and Technology, Gamasa, Mansoura, Dakahlia, Egypt. Die Arbeit nennt 30 Literaturangaben.
Abstract (Originalsprache)
Purpose
To evaluate the effect of different preparation designs and ceramic thicknesses on the fracture resistance and failure mode of maxillary premolars with non‐carious cervical lesions restored with milled lithium disilicate laminate veneers. Materials and Methods Seventy‐eight sound maxillary premolars were randomly assigned to six groups ( n = 13) based on preparation design and thickness: BC3 (0.3 mm buccal reduction), BR3 (same as BC3 with composite resin restoration filling the lesion), BRO3 (same as BR3 and 1 mm occlusal reduction for buccal cusp slopes), BC5, BR5, and BRO5; prepared as contralateral groups but with buccal reduction of 0.5 mm. All specimens were restored with lithium disilicate laminate veneers, subjected to 10,000 thermocycles and 240,000 chewing cycles (49 N), and then loaded to failure at a 45° angle. Data were analyzed using two‐way ANOVA and chi‐square tests ( α = 0.05).
Results
There was a significant main effect of preparation design on fracture resistance ( p < 0.001), whereas ceramic thickness ( p = 0.470) and the interaction between design and thickness ( p = 0.138) did not reach statistical significance. Moreover, there was a significant difference in the failure mode between tested groups ( p < 0.001) with predominant Type II unrepairable failure in the ceramic material, leaving the tooth intact for BRO groups.
Conclusions
All tested designs provided mean fracture resistance values within the physiological bite force range for all tested groups for the premolar region, this must be interpreted alongside the failure mode distribution. BC and BR preparation designs demonstrated a clinically meaningful rate of catastrophic Type IV root fractures, whereas BRO preparations produced predominant cohesive ceramic failure Type II. The thickness of the lithium disilicate laminate veneers, whether 0.3 or 0.5 mm, did not significantly affect fracture resistance or failure patterns.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Department of Prosthodontics, Faculty of Oral and Dental Medicine, Delta University for Science and Technology, Gamasa, Mansoura, Dakahlia, Egypt.
- Faculty of Dentistry, Mansoura University, Mansoura, Dakahlia, Egypt.
ORCID-Profile: Waleed Ahmed Abdelnaby, Amal Abdelsamad Sakrana, Walid Al-Zordk, Mohamed Hamed Ghazy
Zitieren
APA
Abdelnaby, W. A., Sakrana, A. A., Al-Zordk, W., & Ghazy, M. H. (2026). Fracture resistance and failure mode of teeth with non‐carious cervical lesions restored with laminate veneers: Effect of preparation design and restoration thickness. Journal of Prosthodontics. https://doi.org/10.1111/jopr.70191
Vancouver
Abdelnaby WA, Sakrana AA, Al-Zordk W, Ghazy MH. Fracture resistance and failure mode of teeth with non‐carious cervical lesions restored with laminate veneers: Effect of preparation design and restoration thickness. Journal of Prosthodontics. 2026. doi:10.1111/jopr.70191
BibTeX
@article{Abdelnaby2026,
author = {Abdelnaby, Waleed Ahmed and Sakrana, Amal Abdelsamad and Al-Zordk, Walid and Ghazy, Mohamed Hamed},
title = {Fracture resistance and failure mode of teeth with non‐carious cervical lesions restored with laminate veneers: Effect of preparation design and restoration thickness},
journal = {Journal of Prosthodontics},
year = {2026},
doi = {10.1111/jopr.70191}
}
EUVIMED