Fachartikel in der Zeitschrift Journal of Prosthodontics, 2023. Verfasst von Pithiwat Uasuwan und 2 weiteren Autor:innen. Beteiligte Einrichtung: Division of Biomaterials and Prosthodontics Research, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand. Hauptthemen laut MEDLINE: Flexural Strength, Dental Materials. Die Arbeit wurde bisher 14-mal zitiert (Crossref) und nennt 31 Literaturangaben. Gefördert von: Faculty of Dentistry, Khon Kaen University, Ministry of Higher Education, Science, Research and Innovation, Royal Thai Government.
Abstract (Originalsprache)
Purpose
Firing protocols influence the mechanical properties of dental ceramics. This study examined the impact of altering the cooling rate of mono‐ and multilayered 5 mol% yttria‐partially stabilized zirconia (5Y‐PSZ) on their strength. Materials and methods Ninety specimens (width × length × thickness = 10 × 20 × 2 mm) were prepared using 5Y‐PSZ monolayer (Mo: Cercon‐xt) and 5Y‐PSZ multilayered (Mu: Cercon‐xt ML) blocks. Randomly distributed specimens were sintered at the recommended firing schedule for three different categories of cooling rates ( n = 15/group): slow (S: 5°C/min), normal (N: 35°C/min), and fast (F: 70°C/min). A universal testing machine with four‐point bending test was used to measure the flexural strength ( σ ). The microstructure, fracture characteristics, and chemical composition were evaluated by scanning electron microscope and energy‐dispersive spectroscopy. The monoclinic, tetragonal, and cubic phases were investigated using X‐ray diffraction. Two‐way ANOVA and post hoc Bonferroni comparisons were applied to determine the σ , (), and Weibull analysis was performed to determine the Weibull modulus ( m ) and characteristic strength ( σ 0 ).
Results
The highest σ and σ 0 (MPa) were seen for MuN (454.2 ± 62.0, 480.8 ± 62.9) followed by MuS (453.5 ± 52.6, 476.4 ± 54.3) and MoS (451.5 ± 44.5, 471.2 ± 46.6), whereas MuF had the lowest σ and σ 0 (379.8 ± 50.2, 401.6 ± 51.3). The σ value of S‐cooling (452.5 ± 47.9) was higher than those for N‐cooling (443.4 ± 61.3) and F‐cooling (382.3 ± 58.0). The m ‐value for MoS was the highest (11.4 ± 3.6), whereas that for MoF was the lowest (6.1 ± 1.6). Different cooling rates resulted in a significant difference in σ values ( p < 0.05).
Conclusions
S‐ and N‐cooling resulted in significantly higher flexural strength than that obtained by F‐cooling. Increasing the cooling rate of 5Y‐PSZ resulted in smaller grain size, less grain boundary integration, and higher t‐ to m‐transformation, leading to lower strength. Therefore, a slow and normal cooling rate was recommended to achieve the optimum strength for 5Y‐PSZ.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Division of Biomaterials and Prosthodontics Research, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand.
- Department of Prosthodontics, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand.
- Division of Pediatric Dentistry, Department of Preventive Dentistry, Faculty of Dentistry, Khon Kaen University, Khon Kaen, Thailand.
ORCID-Profile: Niwut Juntavee
Förderung
- Faculty of Dentistry, Khon Kaen University
- Ministry of Higher Education, Science, Research and Innovation
- Royal Thai Government
Zitieren
APA
Uasuwan, P., Juntavee, N., & Juntavee, A. (2023). Flexural strength of high yttrium oxide‐doped monochrome and multilayered fully stabilized zirconia upon various sintered cooling rates. Journal of Prosthodontics. https://doi.org/10.1111/jopr.13692
Vancouver
Uasuwan P, Juntavee N, Juntavee A. Flexural strength of high yttrium oxide‐doped monochrome and multilayered fully stabilized zirconia upon various sintered cooling rates. Journal of Prosthodontics. 2023. doi:10.1111/jopr.13692
BibTeX
@article{Uasuwan2023,
author = {Uasuwan, Pithiwat and Juntavee, Niwut and Juntavee, Apa},
title = {Flexural strength of high yttrium oxide‐doped monochrome and multilayered fully stabilized zirconia upon various sintered cooling rates},
journal = {Journal of Prosthodontics},
year = {2023},
doi = {10.1111/jopr.13692}
}
EUVIMED