Hydration Product Evolution and Thermodynamic Modeling of Aluminosilicate Glasses in Supersulfated Cementitious Systems

Jixiang Wang, Bo Liu, Tao Li, Rui Sun, Dongmin Wang, Zhenbo Wang

Journal of the American Ceramic Society · 2026-11 · 109 (11)

DOI: 10.1111/jace.71398 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of the American Ceramic Society, online erschienen am 05.11.2026. Verfasst von Jixiang Wang und 5 weiteren Autor:innen. Die Arbeit nennt 63 Literaturangaben. Gefördert von: National Key Research and Development Program of China, National Natural Science Foundation of China, China Postdoctoral Science Foundation.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Supersulfated cement (SSC) is considered a promising low‐carbon cementitious material. However, the intrinsic characteristics of aluminosilicate glasses and their hydration behavior remain insufficiently understood. This study systematically investigates the hydration reactivity, phase evolution, and thermodynamic properties of synthesized aluminosilicate glasses with representative compositions in SSC systems. Four model glasses with different CaO–Al 2 O 3 –SiO 2 compositions were prepared to represent typical solid waste‐derived precursors, including silica‐rich, slag‐like, alumina‐rich, and high‐Ca/high‐Al glasses. Their hydration behavior was evaluated through X‐ray diffraction, SEM/BSE‐EDS analysis, isothermal calorimetry, and quantitative determination of the glass reaction degree, and thermodynamic modeling was used to predict the equilibrium phase assemblages and to clarify the influence of the glass composition on the hydration products. The results show that the aluminosilicate glass composition and network structure critically control both the hydration reactivity and the hydrate assemblage. The highly polymerized, silica‐rich glass dissolves only to a limited extent, whereas the Ca‐ and Al‐rich glasses react rapidly and form large amounts of ettringite and C‐A‐S‐H. Thermodynamic calculations reveal that the slag‐like and high‐Ca/high‐Al glasses are located within compositional domains that are favorable for the formation of the main binding phases of SSC, mainly ettringite and C‐A‐S‐H gel, whereas the silica‐rich and alumina‐rich glasses show only a limited thermodynamic potential for producing these phases. Experimental observations further indicate that hydration kinetics and local supersaturation can promote the formation of ettringite beyond the equilibrium prediction. Increasing the calcium hydroxide dosage and the curing temperature accelerates hydration, but a higher calcium hydroxide dosage delays the main ettringite precipitation. This work provides theoretical guidance for designing high‐performance, low‐carbon SSC materials through the optimization of the precursor composition.

Förderung

  • National Key Research and Development Program of China
  • National Natural Science Foundation of China
  • China Postdoctoral Science Foundation
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Wang, J., Liu, B., Li, T., Sun, R., Wang, D., & Wang, Z. (2026). Hydration Product Evolution and Thermodynamic Modeling of Aluminosilicate Glasses in Supersulfated Cementitious Systems. Journal of the American Ceramic Society, 109(11). https://doi.org/10.1111/jace.71398

Vancouver

Wang J, Liu B, Li T, Sun R, Wang D, Wang Z. Hydration Product Evolution and Thermodynamic Modeling of Aluminosilicate Glasses in Supersulfated Cementitious Systems. Journal of the American Ceramic Society. 2026;109(11). doi:10.1111/jace.71398

BibTeX
@article{Wang2026,
  author = {Wang, Jixiang and Liu, Bo and Li, Tao and Sun, Rui and Wang, Dongmin and Wang, Zhenbo},
  title = {Hydration Product Evolution and Thermodynamic Modeling of Aluminosilicate Glasses in Supersulfated Cementitious Systems},
  journal = {Journal of the American Ceramic Society},
  year = {2026},
  volume = {109},
  number = {11},
  doi = {10.1111/jace.71398}
}
Kostenlos starten →