Preparation and Mechanical Properties of a Martian‐Regolith‐Based Geopolymer
Journal of the American Ceramic Society · 2026-11 · 109 (11)
DOI: 10.1111/jace.71396 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of the American Ceramic Society, online erschienen am 10.11.2026. Verfasst von Kamran Arshad und 5 weiteren Autor:innen. Die Arbeit nennt 59 Literaturangaben. Gefördert von: National Natural Science Foundation of China.
Abstract (Originalsprache)
Alkali‐cation chemistry critically governs the reaction kinetics, structural evolution, and mechanical performance of regolith‐derived geopolymers, yet the respective roles of Na + and K + remain insufficiently understood. In this study, Martian‐regolith‐based geopolymers activated with five Na/K compositions Na100, Na75K25, Na50K50, Na25K75, and K100 were systematically investigated. Geopolymerization was monitored during the initial reaction stage I (15–45 min) and subsequent curing stage II (0.5–48 h) using FTIR, XRD, PSD, XRF, SEM, 27 Al MAS NMR, and 29 Si MAS NMR, together with compressive testing. The results revealed two overlapping reaction regimes: precursor dissolution and the formation of reactive silicate and aluminate species during the initial stage, followed by polycondensation, network reorganization, and matrix consolidation during curing. FTIR showed a progressive shift of the Si–O–T band toward lower wavenumbers, depletion of terminal hydroxyl groups, and development of Si–O–Al linkages. The 29 Si MAS NMR demonstrated conversion of Q 2 and Q 3 species into highly polymerized Q 4 (3Al) and Q 4 (4Al) environments, with Na25K75 reaching a total Q 4 fraction of 99.51% after curing. Concurrently, 27 Al MAS NMR indicated the progressive incorporation of tetrahedrally coordinated Al into the geopolymer network. Na25K75 exhibited highest compressive strength, reaching 28.5 ± 1.8 MPa in the Mars regolith simulant geopolymer, compared with 13.3 ± 0.8 MPa for Na100, representing an increase of approximately 114%. These findings demonstrate that Na + primarily promotes precursor dissolution, whereas K + facilitates condensation and network stabilization. Their synergistic combination in Na25K75 provides most favorable balance between dissolution and gel formation, establishing a direct relationship among alkali composition, aluminosilicate network connectivity, microstructure densification, and mechanical performance.
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Arshad, K., Peigang, H., Xiaoming, D., Dechang, J., Paolo, C., & Yu, Z. (2026). Preparation and Mechanical Properties of a Martian‐Regolith‐Based Geopolymer. Journal of the American Ceramic Society, 109(11). https://doi.org/10.1111/jace.71396
Vancouver
Arshad K, Peigang H, Xiaoming D, Dechang J, Paolo C, Yu Z. Preparation and Mechanical Properties of a Martian‐Regolith‐Based Geopolymer. Journal of the American Ceramic Society. 2026;109(11). doi:10.1111/jace.71396
BibTeX
@article{Arshad2026,
author = {Arshad, Kamran and Peigang, He and Xiaoming, Duan and Dechang, Jia and Paolo, Colombo and Yu, Zhou},
title = {Preparation and Mechanical Properties of a Martian‐Regolith‐Based Geopolymer},
journal = {Journal of the American Ceramic Society},
year = {2026},
volume = {109},
number = {11},
doi = {10.1111/jace.71396}
}
EUVIMED