Mechanical Properties of High‐Purity, High‐Density NaSICON (Na 1+ x Zr 2 Si x P 3− x O 12 , 2 ≤ x ≤ 2.8)
Journal of the American Ceramic Society · 2026-11 · 109 (11)
DOI: 10.1111/jace.71284 ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of the American Ceramic Society, online erschienen am 05.11.2026. Verfasst von Seneca Stevens und 11 weiteren Autor:innen. Die Arbeit nennt 80 Literaturangaben.
Abstract (Originalsprache)
NaSICON (Na Super Ionic Conductor) ceramics with formula Na 1+ x Zr 2 Si x P 3− x O 12 (NZSP) are leading solid electrolyte candidates for sodium‐based energy storage. However, the mechanical properties governing membrane reliability, namely elastic modulus, hardness, fracture toughness, and flexural strength, have not been systematically characterized across the full composition range, owing to confounding effects from porosity, glassy grain‐boundary phases, and ZrO 2 transformation‐induced and grain‐boundary microcracking in conventionally sintered materials. Here, we report the first comprehensive mechanical characterization of high‐purity (total secondary‐phase content < 10%), fully dense NZSP across x = 2.0–2.8, prepared by rapid induction hot‐pressing of powders prepared by solution‐assisted solid‐state reaction. Hot‐pressed samples achieve relative densities exceeding 99%, nanosized grains (150–200 nm), nanosized ZrO 2 particles, and glass‐free grain boundaries across most compositions. Elastic modulus increases from 109 GPa ( x = 2.0) to 124 GPa ( x = 2.8), attributed to progressive replacement of compliant phosphate units by stiffer silicate groups and the corresponding increase in the stiffer rhombohedral phase. Hardness follows the same trend, rising from 7.20 to 9.61 GPa. Fracture toughness falls between 1.0 and 1.5 MPa·m 1/2 . Biaxial flexure strength reaches a maximum of 195 MPa at x = 2.4. The critical grain size for thermal expansion anisotropy‐driven cracking falls from 9 µm ( x = 2) to 0.5 µm ( x = 3), for both phases above the hot‐pressed grain size at every composition.
Zitieren
APA
Stevens, S., Bhagwat, T. M., Howard, H., Fang, Z., Wang, C., MacLeod, E., Chi, M., Gianola, D. S., Wolfenstine, J., Siegel, D. J., Begley, M., & Sakamoto, J. (2026). Mechanical Properties of High‐Purity, High‐Density NaSICON (Na 1+ x Zr 2 Si x P 3− x O 12 , 2 ≤ x ≤ 2.8). Journal of the American Ceramic Society, 109(11). https://doi.org/10.1111/jace.71284
Vancouver
Stevens S, Bhagwat TM, Howard H, Fang Z, Wang C, MacLeod E, et al. Mechanical Properties of High‐Purity, High‐Density NaSICON (Na 1+ x Zr 2 Si x P 3− x O 12 , 2 ≤ x ≤ 2.8). Journal of the American Ceramic Society. 2026;109(11). doi:10.1111/jace.71284
BibTeX
@article{Stevens2026,
author = {Stevens, Seneca and Bhagwat, Tanmay Mohan and Howard, Hannah and Fang, Zhengwu and Wang, Cathy and MacLeod, Egan and Chi, Miaofang and Gianola, Daniel S. and Wolfenstine, Jeff and Siegel, Donald J. and Begley, Matthew and Sakamoto, Jeff},
title = {Mechanical Properties of High‐Purity, High‐Density NaSICON (Na 1+ x Zr 2 Si x P 3− x O 12 , 2 ≤ x ≤ 2.8)},
journal = {Journal of the American Ceramic Society},
year = {2026},
volume = {109},
number = {11},
doi = {10.1111/jace.71284}
}
EUVIMED