EUVIMEDEUVIMED entdecken
Crossref

Crystal Chemistry and Leaching Behavior of Sn‐Based Hollandite Waste Forms for Cs Immobilization

Mingyang Zhao, Yupeng Jiao, Zhenfeng Tong

Journal of the American Ceramic Society · 2026-07 · 109 (7)

DOI: 10.1111/jace.70960 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of the American Ceramic Society, online erschienen am 07.07.2026. Verfasst von Mingyang Zhao und 2 weiteren Autor:innen. Die Arbeit nennt 54 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Fundamental Research Funds for the Central Universities.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Sn‐containing hollandite has been highlighted by recent machine learning‐guided design as a promising host for radioactive cesium (Cs), yet waste form validation remains limited. Here, a Cs‐bearing Sn‐based hollandite series, (Ba,Cs) 1.66 (Fe,Sn) 8 O 16 , was synthesized in air by solid‐state reaction, with hollandite formation at 1125°C followed by pressureless sintering at 1200°C. x‐Ray diffraction confirms hollandite as the major phase across the series, with minor Ba‐bearing secondary phases only at low Cs contents. Rietveld refinement reveals anisotropic lattice expansion and a tetragonal‐to‐monoclinic symmetry change at the Cs‐rich end member, accompanied by progressive tightening of tunnel descriptors, indicating a Sn‐specific Cs accommodation response distinct from many Ti‐based hollandites. Chemical durability was evaluated by monolithic leaching in deionized water at 90°C. At Cs loadings up to ∼17 wt%, 7‐day Cs release is comparable to representative Ti‐based hollandites tested under similar conditions. Sn exhibits ultralow normalized release, while Cs and Ba show higher release without detectable degradation of the hollandite matrix. Extended 28‐day interval leaching on Ba 0.8 Cs 0.86 Fe 2.46 Sn 5.54 O 16 (HS2) and Ba 0.4 Cs 1.26 Fe 2.06 Sn 5.94 O 16 (HS3) separates rapid early wash‐off from slower, diffusion‐controlled release. By 14–28 days, Cs and Ba leaching rates converge to ∼2–4 × 10 −2 g·m −2 ·day −1 , with effective diffusion coefficients of ∼1–2 × 10 −11 cm 2 /s and leaching indices of ∼11. Benchmarking against Ti‐based hollandites places the Sn‐based series within a competitive loading–durability window under a comparatively mild processing route, supporting Sn‐based hollandite as a readily fabricated candidate for high‐loading Cs immobilization.

Förderung

  • National Natural Science Foundation of China
  • Fundamental Research Funds for the Central Universities

Zitieren

APA

Zhao, M., Jiao, Y., & Tong, Z. (2026). Crystal Chemistry and Leaching Behavior of Sn‐Based Hollandite Waste Forms for Cs Immobilization. Journal of the American Ceramic Society, 109(7). https://doi.org/10.1111/jace.70960

Vancouver

Zhao M, Jiao Y, Tong Z. Crystal Chemistry and Leaching Behavior of Sn‐Based Hollandite Waste Forms for Cs Immobilization. Journal of the American Ceramic Society. 2026;109(7). doi:10.1111/jace.70960

BibTeX
@article{Zhao2026,
  author = {Zhao, Mingyang and Jiao, Yupeng and Tong, Zhenfeng},
  title = {Crystal Chemistry and Leaching Behavior of Sn‐Based Hollandite Waste Forms for Cs Immobilization},
  journal = {Journal of the American Ceramic Society},
  year = {2026},
  volume = {109},
  number = {7},
  doi = {10.1111/jace.70960}
}
Kostenlos starten →