Fachartikel in der Zeitschrift Photobiomodulation, Photomedicine, and Laser Surgery, online erschienen am 17.10.2024. Verfasst von Fahad Alkhudhairy. Beteiligte Einrichtung: Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh, Saudi Arabia. Hauptthemen laut MEDLINE: Chitosan, Methylene Blue, Phosphoric Acids, Dentin. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 57 Literaturangaben.
Abstract (Originalsprache)
Aim
To prepare experimental adhesive (EA) with 1% and without chitosan nanoparticles on dentin conditioned with a conventional technique phosphoric acid (PA) compared with two different contemporary techniques: photodynamic therapy (PDT) and femtosecond laser (FSL).
Method
The methodology consisted of synthesis of EA and 1% chitosan-modified adhesive (CMA). Scanning electron microscopy, dentin adhesive interface assessment, energy-dispersive spectroscopy, shear bond strength (SBS), degree of conversion (DC), and bond failure were assessed. Teeth were selected, disinfected, and mounted in acrylic up to the cementoenamel junction. Occlusal enamel was removed and teeth were randomly allocated into groups and conditioned. These included Group 1: samples treated with PA; Group 2: specimens conditioned with methylene blue photosensitizer (MBP) activated by PDT; and Group 3: samples conditioned with FSL. Following different conditioning regimes, specimens were bonded using 1% CMA and EA. The composite buildup was followed by SBS testing and a bond failure assessment. DC was assessed for both EA and CMA. Analysis of variance and Tukey’s post hoc test were used to compare the mean and standard deviation of SBS and DC in different experimental groups, with a significance level of p < 0.05.
Results
Dentin pretreated with etch and rinse demonstrated the highest bond strength with 1% CMA. Dentin conditioned with MBP activated by PDT and bonded to EA showed the lowest bond scores. Overall SBS values of 1% CMA were better than EA irrespective of the conditioning regime of dentin. The DC was higher in EA adhesive. This was followed by DC in 1% CMA. DC in EA was found to be comparable with 1% CMA.
Conclusions
PA remains the gold standard for dentin conditioning. The incorporation of 1% chitosan in adhesive improves SBS and results in no change in DC. The use of FSL in dentin conditioning can be used as an alternative approach as it results in SBS within acceptable limits. The study was approved by the ethical board of King Saud University.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Restorative Dental Sciences Department, College of Dentistry, King Saud University, Riyadh, Saudi Arabia.
Zitieren
APA
Alkhudhairy, F. (2024). Experimental and Chitosan-Infused Adhesive with Dentin Pretreated with Femtosecond Laser, Methylene Blue-Activated Low-Level Laser, and Phosphoric Acid. Photobiomodulation, Photomedicine, and Laser Surgery, 42(10), 634-642. https://doi.org/10.1089/pho.2024.0077
Vancouver
Alkhudhairy F. Experimental and Chitosan-Infused Adhesive with Dentin Pretreated with Femtosecond Laser, Methylene Blue-Activated Low-Level Laser, and Phosphoric Acid. Photobiomodulation, Photomedicine, and Laser Surgery. 2024;42(10):634-642. doi:10.1089/pho.2024.0077
BibTeX
@article{Alkhudhairy2024,
author = {Alkhudhairy, Fahad},
title = {Experimental and Chitosan-Infused Adhesive with Dentin Pretreated with Femtosecond Laser, Methylene Blue-Activated Low-Level Laser, and Phosphoric Acid},
journal = {Photobiomodulation, Photomedicine, and Laser Surgery},
year = {2024},
volume = {42},
number = {10},
pages = {634--642},
doi = {10.1089/pho.2024.0077}
}
EUVIMED