Sintering temperature effect on the electrical conductivity of core–shell structured BaCe 0.8 Gd 0.2 O 3− δ @Ce 0.8 Gd 0.2 O 2− δ ceramic
Materials Research Express · 28.04.2026 · 13 (8) · 086301
DOI: 10.1088/2053-1591/ae5d95 ↗Kurz gefasst
Fachartikel in der Zeitschrift Materials Research Express, online erschienen am 24.04.2026. Verfasst von Hao Wang und 5 weiteren Autor:innen. Die Arbeit nennt 27 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China, Yunnan Fundamental Research Projects.
Abstract (Originalsprache)
In this study, the core–shell structured BaCe 0.8 Gd 0.2 O 3− δ @Ce 0.8 Gd 0.2 O 2− δ (BCG@GDC) powders were synthesized by co-precipitation method, and the corresponding core–shell BCG@GDC ceramics were prepared through conventional sintering at 1400 °C, 1500 °C and 1600 °C. XRD and SEM analyses confirm that the synthesized BCG@GDC powders and ceramics are only composed of BCG and GDC phases. A TEM analysis on the BCG@GDC powders demonstrates that a layer of GDC shell with a thickness of about 9.4 nm is wrapped on the surface of BCG core with an average size of 49 nm. Compared with core–shell structured Ce 0.8 Gd 0.2 O 2− δ @BaCe 0.8 Gd 0.2 O 3− δ (GDC@BCG) ceramics, in which the BCG phase is wrapped by GDC phase, the relative density of BCG@GDC ceramics sintered at 1600 °C in this study rises by 4%. This leads to an enhancement of the electrical conductivity of BCG@GDC (1.9 × 10 −2 S cm −1 at 600 °C in air), significantly higher than that of GDC@BCG (1.0 × 10 −2 S cm −1 at 600 °C in air). The rise in sintering temperatures can contribute to the improvement of the relative density as well as the electrical conductivity of the core–shell structured BCG@GDC ceramics.
Förderung
- National Natural Science Foundation of China
- Yunnan Fundamental Research Projects
Zitieren
APA
Wang, H., Meng, B., Ping, X., Yang, Q., Zhang, W., & Fang, C. (2026). Sintering temperature effect on the electrical conductivity of core–shell structured BaCe 0.8 Gd 0.2 O 3− δ @Ce 0.8 Gd 0.2 O 2− δ ceramic. Materials Research Express, 13(8), 086301. https://doi.org/10.1088/2053-1591/ae5d95
Vancouver
Wang H, Meng B, Ping X, Yang Q, Zhang W, Fang C. Sintering temperature effect on the electrical conductivity of core–shell structured BaCe 0.8 Gd 0.2 O 3− δ @Ce 0.8 Gd 0.2 O 2− δ ceramic. Materials Research Express. 2026;13(8):086301. doi:10.1088/2053-1591/ae5d95
BibTeX
@article{Wang2026,
author = {Wang, Hao and Meng, Bin and Ping, Xinyu and Yang, Qingqing and Zhang, Wenlong and Fang, Congcong},
title = {Sintering temperature effect on the electrical conductivity of core–shell structured BaCe 0.8 Gd 0.2 O 3− δ @Ce 0.8 Gd 0.2 O 2− δ ceramic},
journal = {Materials Research Express},
year = {2026},
volume = {13},
number = {8},
pages = {086301},
doi = {10.1088/2053-1591/ae5d95}
}