Genipin-crosslinked aligned PCL/gelatin/chitosan nanofibre scaffolds functionalised with PEDOT:PSS: electrical characterisation and cytotoxicity assessment using L929 fibroblasts

Darius Čiužas, Vilma Petrikaitė

Biomedical Materials · 18.11.2026

DOI: 10.1088/1748-605x/aec3fe ↗

Kurz gefasst

Fachartikel in der Zeitschrift Biomedical Materials, online erschienen am 18.11.2026. Verfasst von Darius Čiužas und 1 weiteren Autor:innen.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Electrospun polycaprolactone/gelatin/chitosan (PCL/GE/CS) composite nanofibre scaffolds are attractive for tissue engineering. However, their intrinsic electrical insulation limits electroactive applications. Here, we report aligned PCL/GE/CS nanofibre scaffolds fabricated using an acetic acid/acetone-based electrospinning route that avoids chlorinated solvents, crosslinked with genipin and subsequently functionalised by PEDOT:PSS dip-coating.
The optimised PCL/GE/CS stock-solution mixing ratio of 80:10:10 (v/v/v), corresponding to final polymer concentrations of 16.0, 1.0 and 0.2% (w/v), produced uniform, bead-free aligned fibres with an average diameter of 356 ± 86 nm. Genipin crosslinking improved aqueous stability, with the scaffolds retaining approximately 98.9 ± 0.2% of their initial dry mass after 14 days in PBS compared with 95.4 ± 0.4% for the corresponding non-crosslinked PCL/GE/CS scaffolds, and reduced the 24 h swelling ratio from 440.8 ± 7.7% to 395.4 ± 9.3%. Subsequent genipin crosslinking and PEDOT:PSS coating slightly increased fibre diameter while preserving the aligned architecture. Surface characterisation confirmed PEDOT:PSS deposition by FTIR and SEM-EDX sulphur mapping. Wettability improved markedly: the water contact angle decreased from 143.2 ± 1.2° for PCL to 104.2 ± 2.4° for PCL/GE/CS and to 41.6 ± 6.2° after genipin crosslinking, while PEDOT:PSS-coated mats showed rapid droplet absorption. The conductivity was anisotropic, reaching 2.22 ± 0.15 S/m parallel to fibre alignment and 1.12 ± 0.06 S/m perpendicular to the fibre axis. 
In vitro studies with L929 fibroblasts showed no extract-mediated cytotoxicity under the tested conditions. Direct cell culture demonstrated increasing MTT metabolic activity from day 1 to day 7, while representative Live/Dead and DAPI/phalloidin images indicated sustained cell survival, attachment and cytoskeletal organisation. These findings demonstrate measurable electrical functionality together with L929 fibroblast compatibility and support further investigation of the scaffold as a candidate platform for electroactive tissue-engineering studies.

Zitieren

APA

Čiužas, D., & Petrikaitė, V. (2026). Genipin-crosslinked aligned PCL/gelatin/chitosan nanofibre scaffolds functionalised with PEDOT:PSS: electrical characterisation and cytotoxicity assessment using L929 fibroblasts. Biomedical Materials. https://doi.org/10.1088/1748-605x/aec3fe

Vancouver

Čiužas D, Petrikaitė V. Genipin-crosslinked aligned PCL/gelatin/chitosan nanofibre scaffolds functionalised with PEDOT:PSS: electrical characterisation and cytotoxicity assessment using L929 fibroblasts. Biomedical Materials. 2026. doi:10.1088/1748-605x/aec3fe

BibTeX
@article{iuas2026,
  author = {Čiužas, Darius and Petrikaitė, Vilma},
  title = {Genipin-crosslinked aligned PCL/gelatin/chitosan nanofibre scaffolds functionalised with PEDOT:PSS: electrical characterisation and cytotoxicity assessment using L929 fibroblasts},
  journal = {Biomedical Materials},
  year = {2026},
  doi = {10.1088/1748-605x/aec3fe}
}
Kostenlos starten →