Fachartikel in der Zeitschrift Physica Scripta, online erschienen am 30.03.2026. Verfasst von Zhiyou He und 2 weiteren Autor:innen. Die Arbeit nennt 58 Literaturangaben. Gefördert von: Tianshan Innovation Team Program of Xinjiang Uygur Autonomous Region, Fundamental Research Funds for Autonomous Region Universities, Natural Science Foundation of Xinjiang Uygur Autonomous Region.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

For 3D-printed silica ceramics, addressing challenges such as insufficient densification, low mechanical strength, and deformation or cracking is essential for advancing their application in high-end fields including aerospace and electronic information technologies. As a key processing parameter in the fabrication of 3D-printed ceramics, the debinding heating rate can significantly influence ceramic performance by regulating binder decomposition, gas release, and the subsequent sintering behavior of green bodies. Therefore, investigating the effect of this parameter on the properties of silica ceramics holds substantial practical importance. In this study, silica powders were used as raw materials, and ceramic green bodies were fabricated via photopolymerization-based 3D printing. A gradient of debinding heating rates from 2 to 7 °C min −1 was applied, followed by sintering, to evaluate their influence on the final ceramic performance. The samples were characterized through flexural testing, open porosity and bulk density measurements, shrinkage analysis, and microstructural observations. The results show that the sample debinded at 3 °C min −1 exhibited the highest flexural strength (10.80 ± 0.46 MPa). However, the overall performance was optimized at 7 °C min −1 , where the sample maintained a high flexural strength (10.69 ± 0.35 MPa), while achieving the lowest open porosity (5.20 ± 0.06%) and the highest bulk density (2.19 ± 0.01 g cm −3 ). The shrinkage in length, width, and height reached 11.55 ± 0.55%, 11.75 ± 0.60%, and 19.77 ± 0.51%, respectively, indicating a relatively stable shrinkage behavior. Conversely, the sample processed at 5 °C min −1 showed the poorest performance, with a reduced flexural strength (7.59 ± 0.26 MPa), increased open porosity (6.23 ± 0.07%), and decreased bulk density (2.15 ± 0.01 g cm −3 ). This study provides theoretical support for optimizing the debinding process of 3D-printed silica ceramics and offers practical insights for improving their overall performance and industrial application potential.

Förderung

  • Tianshan Innovation Team Program of Xinjiang Uygur Autonomous Region
  • Fundamental Research Funds for Autonomous Region Universities
  • Natural Science Foundation of Xinjiang Uygur Autonomous Region

Zitieren

APA

He, Z., Li, H., & Sun, S. (2026). Improved 3D printed silica ceramics via the optimization of heating rates during debinding. Physica Scripta, 101(13), 135904. https://doi.org/10.1088/1402-4896/ae542a

Vancouver

He Z, Li H, Sun S. Improved 3D printed silica ceramics via the optimization of heating rates during debinding. Physica Scripta. 2026;101(13):135904. doi:10.1088/1402-4896/ae542a

BibTeX
@article{He2026,
  author = {He, Zhiyou and Li, He and Sun, Shengxian},
  title = {Improved 3D printed silica ceramics via the optimization of heating rates during debinding},
  journal = {Physica Scripta},
  year = {2026},
  volume = {101},
  number = {13},
  pages = {135904},
  doi = {10.1088/1402-4896/ae542a}
}
Kostenlos starten →