EUVIMEDEUVIMED entdecken
Crossref

Transverse-load-induced electromechanical degradation and damage evolution in TSSC REBCO cables

Jinxin Li, Xianfeng Xu, Zekun Jin, Shu Tao, Yi Shi

Superconductor Science and Technology · 01.10.2026 · 39 (10) · 105051

DOI: 10.1088/1361-6668/aeb830 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Superconductor Science and Technology, online erschienen am 04.11.2026. Verfasst von Jinxin Li und 4 weiteren Autor:innen. Die Arbeit nennt 49 Literaturangaben. Gefördert von: Comprehensive Research Facility for Fusion Technology Program of China, National Natural Science Foundation of China.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Large transverse Lorentz forces in high-field superconducting magnets pose severe challenges to the mechanical integrity and operational reliability of REBa 2 Cu 3 O 7 − δ (REBCO) conductors. However, cable-scale electromechanical studies above 10 3 kN m −1 remain rare, and the mechanics-to-performance degradation pathway of mechanically heterogeneous, solder-encapsulated REBCO cables remains poorly understood, impeding technological advancement. In this study, cryogenic electromechanical experiments at 77 K were integrated with three-dimensional finite-element simulations to quantify the monotonic and cyclic transverse-load responses of twisted stacked slotted-core (TSSC) REBCO cables and provide mechanics-based interpretations of damage susceptibility. Monotonic tests reveal a pronounced loading-orientation effect: at 95% critical-current retention, the cable sustains 2080 kN m −1 under 0° loading, approximately 33% higher than the 1560 kN m −1 sustained under 45° loading. Simulations further link this difference to orientation-dependent load redistribution, resulting in distinct spatial patterns of local plasticity and solder damage initiation, together with corresponding variations in the mixed-mode interlaminar damage-driving index near the REBCO tape edges. Additionally, cyclic tests reveal load-level-dependent degradation behavior: at 1500 kN m −1 , the cable exhibits a three-stage degradation process with accelerated degradation after approximately 900 cycles, whereas at 1375 kN m −1 , the critical current remains nearly unchanged after 1000 cycles. Moreover, cross-sectional observations identify solder voids and insufficiently filled regions as processing-induced defects, while defect-containing finite-element models show that these defects amplify local stresses and disrupt load-transfer continuity. These findings establish a contact–plasticity–damage failure pathway and provide mechanics-based guidance for defect control and structural optimization of reliable TSSC conductors.

Förderung

  • Comprehensive Research Facility for Fusion Technology Program of China
  • National Natural Science Foundation of China

Zitieren

APA

Li, J., Xu, X., Jin, Z., Tao, S., & Shi, Y. (2026). Transverse-load-induced electromechanical degradation and damage evolution in TSSC REBCO cables. Superconductor Science and Technology, 39(10), 105051. https://doi.org/10.1088/1361-6668/aeb830

Vancouver

Li J, Xu X, Jin Z, Tao S, Shi Y. Transverse-load-induced electromechanical degradation and damage evolution in TSSC REBCO cables. Superconductor Science and Technology. 2026;39(10):105051. doi:10.1088/1361-6668/aeb830

BibTeX
@article{Li2026,
  author = {Li, Jinxin and Xu, Xianfeng and Jin, Zekun and Tao, Shu and Shi, Yi},
  title = {Transverse-load-induced electromechanical degradation and damage evolution in TSSC REBCO cables},
  journal = {Superconductor Science and Technology},
  year = {2026},
  volume = {39},
  number = {10},
  pages = {105051},
  doi = {10.1088/1361-6668/aeb830}
}