Suppressing Zn pulverization with three-dimensional inert-cation diversion dam for long-life Zn metal batteries
Proceedings of the National Academy of Sciences · 20.02.2024 · 121 (8)
DOI: 10.1073/pnas.2317796121 ↗Kurz gefasst
Fachartikel in der Zeitschrift Proceedings of the National Academy of Sciences, online erschienen am 12.02.2024. Verfasst von Xuelong Liao und 12 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Advanced Energy Materials Chemistry (Ministry of Education), Renewable Energy Conversion and Storage Center, Collaborative Innovati…. Die Arbeit wurde bisher 58-mal zitiert (Crossref) und nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: Ministry of Science and Technology of China, MOST | National Natural Science Foundation of China (NSFC).
Abstract (Originalsprache)
Tremendous attention has been paid to the water-associated side reactions and zinc (Zn) dendrite growth on the electrode–electrolyte interface. However, the Zn pulverization that can cause continuous depletion of active Zn metal and exacerbate hydrogen evolution is severely neglected. Here, we disclose that the excessive Zn feeding that causes incomplete crystallization is responsible for Zn pulverization formation through analyzing the thermodynamic and kinetics process of Zn deposition. On the basis, we introduce 1-ethyl-3-methylimidazolium cations (EMIm + ) into the electrolyte to form a Galton-board-like three-dimensional inert-cation (3DIC) region. Modeling test shows that the 3DIC EMIm + can induce the Zn 2+ flux to follow in a Gauss distribution, thus acting as elastic sites to buffer the perpendicular diffusion of Zn 2+ and direct the lateral diffusion, thus effectively avoiding the local Zn 2+ accumulation and irreversible crystal formation. Consequently, anti-pulverized Zn metal deposition behavior is achieved with an average Coulombic efficiency of 99.6% at 5 mA cm −2 over 2,000 cycles and superb stability in symmetric cell over 1,200 h at −30 °C. Furthermore, the Zn||KVOH pouch cell can stably cycle over 1,200 cycles at 2 A g −1 and maintain a capacity of up to 12 mAh.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Key Laboratory of Advanced Energy Materials Chemistry (Ministry of Education), Renewable Energy Conversion and Storage Center, Collaborative Innovation Center of Chemical Science and Engineering (Tianjin), College of Ch…
ORCID-Profile: Shan Chen, Jialei Chen, Huan Wang
Förderung
- Ministry of Science and Technology of China
- MOST | National Natural Science Foundation of China (NSFC)
Zitieren
APA
Liao, X., Chen, S., Chen, J., Li, Y., Wang, W., Lu, T., Chen, Z., Cao, L., Wang, Y., Huang, R., Sun, X., Lv, R., & Wang, H. (2024). Suppressing Zn pulverization with three-dimensional inert-cation diversion dam for long-life Zn metal batteries. Proceedings of the National Academy of Sciences, 121(8). https://doi.org/10.1073/pnas.2317796121
Vancouver
Liao X, Chen S, Chen J, Li Y, Wang W, Lu T, et al. Suppressing Zn pulverization with three-dimensional inert-cation diversion dam for long-life Zn metal batteries. Proceedings of the National Academy of Sciences. 2024;121(8). doi:10.1073/pnas.2317796121
BibTeX
@article{Liao2024,
author = {Liao, Xuelong and Chen, Shan and Chen, Jialei and Li, Youzeng and Wang, Wei and Lu, Tiantian and Chen, Zhuo and Cao, Lixin and Wang, Yaxin and Huang, Rong and Sun, Xiaoting and Lv, Runyu and Wang, Huan},
title = {Suppressing Zn pulverization with three-dimensional inert-cation diversion dam for long-life Zn metal batteries},
journal = {Proceedings of the National Academy of Sciences},
year = {2024},
volume = {121},
number = {8},
doi = {10.1073/pnas.2317796121}
}
EUVIMED