Si-implanted ohmic contacts with modulated pulse activation annealing for down-scaled RF GaN HEMTs

Amer Bassal, Ali Koyucuoglu, Andreas Thies, Ina Ostermay, Pallabi Paul, Serguei Chevtchenko, Oliver Hilt

Journal of Applied Physics · 21.07.2026 · 140 (3)

DOI: 10.1063/5.0331948 ↗

Kurz gefasst

Fachartikel in der Zeitschrift Journal of Applied Physics, online erschienen am 16.07.2026. Verfasst von Amer Bassal und 6 weiteren Autor:innen. Die Arbeit nennt 69 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Bundesministerium für Forschung, Technologie und Raumfahrt, HORIZON EUROPE Framework Programme.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

A modulated pulse annealing method combined with an Al2O3/SiNx annealing cap is utilized for activating implanted Si in n+ ohmic contacts for AlGaN/GaN HEMTs. The objective is to prevent GaN decomposition during annealing and to reduce the alloying temperature of ohmic contacts. This enables the alloying of SiNx-encapsulated contacts for obtaining smooth ohmic contact edges, which is important for downscaled Ka/K-band HEMTs with a short gate–source distance. Al2O3 functions as a diffusion barrier against nitrogen, and SiNx protects the epitaxial layer stack during cap etching and prevents GaN decomposition due to the loss of N. Furthermore, the Al2O3/SiNx cap acts as a retardation layer for Si implantation to achieve a maximum Si concentration in the GaN channel under the AlGaN barrier. Before activation annealing, H is outgassed from the amorphous Al2O3 at 500 °C, which is then crystallized at 900 °C for enhancing its strength. Then it follows the modulated pulsed activation annealing with five pulses peaking at 1250 °C, four pulses at 1300 °C, and one at 1325 °C. The Al2O3/SiNx cap is then removed with dry and wet etching to leave a clean surface, before the deposition of a Ti-based ohmic contact metal. At an implantation dose of 3.5 × 1015 cm−2, 27% activation is achieved without any GaN decomposition, providing a contact resistance of 0.32 Ω mm after contact alloying only at 650 °C for 5 min.

Förderung

  • Bundesministerium für Forschung, Technologie und Raumfahrt
  • HORIZON EUROPE Framework Programme

Zitieren

APA

Bassal, A., Koyucuoglu, A., Thies, A., Ostermay, I., Paul, P., Chevtchenko, S., & Hilt, O. (2026). Si-implanted ohmic contacts with modulated pulse activation annealing for down-scaled RF GaN HEMTs. Journal of Applied Physics, 140(3). https://doi.org/10.1063/5.0331948

Vancouver

Bassal A, Koyucuoglu A, Thies A, Ostermay I, Paul P, Chevtchenko S, et al. Si-implanted ohmic contacts with modulated pulse activation annealing for down-scaled RF GaN HEMTs. Journal of Applied Physics. 2026;140(3). doi:10.1063/5.0331948

BibTeX
@article{Bassal2026,
  author = {Bassal, Amer and Koyucuoglu, Ali and Thies, Andreas and Ostermay, Ina and Paul, Pallabi and Chevtchenko, Serguei and Hilt, Oliver},
  title = {Si-implanted ohmic contacts with modulated pulse activation annealing for down-scaled RF GaN HEMTs},
  journal = {Journal of Applied Physics},
  year = {2026},
  volume = {140},
  number = {3},
  doi = {10.1063/5.0331948}
}
Kostenlos starten →