Endocrowns for Rehabilitation of Anterior Teeth: In Vitro Mechanical Analysis
European Journal of Dentistry · 01.05.2026 · 20 (02) · 645-653
DOI: 10.1055/s-0045-1811715 ↗Kurz gefasst
Fachartikel in der Zeitschrift European Journal of Dentistry, erschienen am 01.05.2026. Verfasst von Alison Flávio Campos Dos Santos und 5 weiteren Autor:innen. Beteiligte Einrichtung: Postgraduate Program in Health Sciences, University of Taubaté, Taubaté, Brazil. Die Arbeit nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: São Paulo Research Foundation.
Abstract (Originalsprache)
This article evaluates the fracture load after mechanical cycling of severely damaged endodontically treated teeth restored with: (1) fiber post, composite resin core, and lithium disilicate (LD) crown; (2) individually fabricated LD post-core and LD crown; (3) LD endocrown; or (4) resin matrix ceramic endocrown. Sixty bovine roots were endodontically treated and prepared for intraradicular retention at depths of 10 or 5 mm. Fiber posts or individually fabricated LD post-cores were cemented into 10-mm-deep prepared root canals. LD crowns were manufactured and cemented onto the cores. Endocrowns (LD or resin matrix ceramic) were fabricated and cemented into 5-mm-deep prepared roots. All samples (n = 15) were subjected to mechanical cycling (1 × 106 cycles at 100 N and 4 Hz), followed by fracture load testing and failure mode analysis. Data were subjected to Kruskal–Wallis followed by Dwass-Steel-Critchlow-Fligner test (α = 0.05). The LD post-core group exhibited seven failures regarding endodontic retention during mechanical cycling and showed the lowest fracture load (192.9 N; p = 0.021). The highest fracture load was observed in the resin matrix ceramic endocrown group (713.9 N), with three catastrophic failures (root fracture). The fiber post-resin core-crown group presented the lowest number of failures during fatigue test (13%) and the lowest number of catastrophic failures (13% root fracture). The improved bonding potential of resin matrix ceramic endocrowns may contribute to higher fracture resistance and enhanced survival under mechanical fatigue compared to LD post-core systems. Resin matrix ceramic endocrowns are an option for restoring anterior severely damaged endodontically treated teeth, with the highest load to failure. However, the conventional post-core-crown strategy demonstrated lower number of failures during fatigue and lowest number of catastrophic failures (root fracture).
Autor:innen und Institutionen
- Postgraduate Program in Health Sciences, University of Taubaté, Taubaté, Brazil.
- Department of Clinical Sciences, College of Dentistry, Ajman University, Ajman, United Arab Emirates.
- Centre of Medical and Bio-allied Health Sciences Research, Ajman, United Arab Emirates.
- Department of Dentistry, University of Taubaté, Taubaté, Brazil.
ORCID-Profile: Kusai Baroudi
Förderung
- São Paulo Research Foundation
Zitieren
APA
Santos, A. F. C. D., Baroudi, K., Almaghribi, R. Y., Concílio, L. R. S., Abreu, R. C. G., & Amaral, M. (2026). Endocrowns for Rehabilitation of Anterior Teeth: In Vitro Mechanical Analysis. European Journal of Dentistry, 20(02), 645-653. https://doi.org/10.1055/s-0045-1811715
Vancouver
Santos AFCD, Baroudi K, Almaghribi RY, Concílio LRS, Abreu RCG, Amaral M. Endocrowns for Rehabilitation of Anterior Teeth: In Vitro Mechanical Analysis. European Journal of Dentistry. 2026;20(02):645-653. doi:10.1055/s-0045-1811715
BibTeX
@article{Santos2026,
author = {Santos, Alison Flávio Campos Dos and Baroudi, Kusai and Almaghribi, Rama Yassin and Concílio, Laís Regiane Silva and Abreu, Regina Clara Gambaro de and Amaral, Marina},
title = {Endocrowns for Rehabilitation of Anterior Teeth: In Vitro Mechanical Analysis},
journal = {European Journal of Dentistry},
year = {2026},
volume = {20},
number = {02},
pages = {645--653},
doi = {10.1055/s-0045-1811715}
}
EUVIMED