Characterization of Polyvinyl Alcohol–Collagen–Hydroxyapatite Composite Membrane from Lates calcarifer Scales for Guided Tissue and Bone Regeneration

Yessy Ariesanti iD, Putri Graesya Melani Octavianus iD, Annisa Tri Handayani iD, Basril Abbas iD

European Journal of Dentistry · 01.10.2023 · 17 (04) · 1153-1162

DOI: 10.1055/s-0042-1759488 ↗

Kurz gefasst

Fachartikel in der Zeitschrift European Journal of Dentistry, erschienen am 01.10.2023. Verfasst von Yessy Ariesanti und 3 weiteren Autor:innen. Beteiligte Einrichtung: Department of Oral and Maxillofacial Surgery, Faculty of Dentistry, Universitas Trisakti, Jakarta, Indonesia. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Objective

To determine the chemical structure, tensile strength, porosity, and degradability of polyvinyl alcohol (PVA)–collagen–hydroxyapatite (HA) composite membranes for guided tissue and bone regeneration. Materials and Methods The PVA–collagen–HA composite membrane was divided into three groups: the group without irradiation, the group with 15 kGy irradiation, and 25 kGy irradiation. Each group was tested for chemical structure with Fourier-transform infrared (FT-IR) at a wavelength of 400 to 4,000 cm−1. Tensile strength test was tested in dry and wet conditions with the standard method of American Standard Testing Mechanical (ASTM) D638, and porosity using scanning electron microscope and analyzed using ImageJ software. Degradability test immersed in a solution of phosphate-buffered saline. Data were analyzed using analysis of variance (ANOVA) and Tukey's test.

Results

FT-IR test before and after storage for 30 days on three media showed a stable chemical structure with the same functional groups. ANOVA analysis showed a significant difference (p < 0.05) in the dry condition (p = 0.006), Tukey's test showed a significant difference in the 15 kGy and 25 kGy irradiated groups (p = 0.005), but the groups without irradiation had no significant difference with the 15 kGy (p = 0.285) and 25 kGy (p = 0.079) irradiation groups. In wet conditions, there was no significant difference (p > 0.05) in each group (p = 373). The size of the porosity in the group without irradiation, 15 kGy irradiation, and 25 kGy irradiation showed a size of 4.65, 6.51, and 8.08 m, respectively. The degradability test showed a decrease in weight in each group, with the total weight of the membrane being completely degraded from the most degraded to the least: the groups without irradiation, 15 kGy irradiation, and 25 kGy irradiation. The ANOVA test on the degradability test shows significant (p < 0.05) in the PVA–collagen–HA composite membrane group over time intervals (p = 0.000). Tukey's post hoc test showed a significant difference (p < 0.05) after 1 week between the groups without irradiation with 15 kGy (p = 0.023).

Conclusion

PVA–collagen–HA composite membrane has a stable chemical structure, optimal tensile strength, porosity, and ideal degradability as guided bone regeneration and guided tissue regeneration.

Autor:innen und Institutionen

  • Department of Oral and Maxillofacial Surgery, Faculty of Dentistry, Universitas Trisakti, Jakarta, Indonesia.
  • Undergraduate Program, Faculty of Dentistry, Universitas Trisakti, Jakarta, Indonesia.
  • National Research and Innovation Agency (BRIN), Jakarta, Indonesia.

ORCID-Profile: Yessy Ariesanti, Putri Graesya Melani Octavianus, Annisa Tri Handayani, Basril Abbas

Zitieren

APA

Ariesanti, Y., Octavianus, P. G. M., Handayani, A. T., & Abbas, B. (2023). Characterization of Polyvinyl Alcohol–Collagen–Hydroxyapatite Composite Membrane from Lates calcarifer Scales for Guided Tissue and Bone Regeneration. European Journal of Dentistry, 17(04), 1153-1162. https://doi.org/10.1055/s-0042-1759488

Vancouver

Ariesanti Y, Octavianus PGM, Handayani AT, Abbas B. Characterization of Polyvinyl Alcohol–Collagen–Hydroxyapatite Composite Membrane from Lates calcarifer Scales for Guided Tissue and Bone Regeneration. European Journal of Dentistry. 2023;17(04):1153-1162. doi:10.1055/s-0042-1759488

BibTeX
@article{Ariesanti2023,
  author = {Ariesanti, Yessy and Octavianus, Putri Graesya Melani and Handayani, Annisa Tri and Abbas, Basril},
  title = {Characterization of Polyvinyl Alcohol–Collagen–Hydroxyapatite Composite Membrane from Lates calcarifer Scales for Guided Tissue and Bone Regeneration},
  journal = {European Journal of Dentistry},
  year = {2023},
  volume = {17},
  number = {04},
  pages = {1153--1162},
  doi = {10.1055/s-0042-1759488}
}
Kostenlos starten →