Hydrogen defects in LaBi 2 O 4 X (X = Cl, Br, and I) Sillén oxyhalide phases and their impacts on ionic transport
Journal of Materials Chemistry A · 2026 · 14 (23) · 14445-14453
DOI: 10.1039/d5ta09720g ↗Kurz gefasst
Fachartikel in der Zeitschrift Journal of Materials Chemistry A, 2026. Verfasst von ShinYoung Kang und 3 weiteren Autor:innen. Die Arbeit nennt 31 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 3.0). Gefördert von: Hydrogen and Fuel Cell Technologies Office, Office of Energy Efficiency and Renewable Energy, Lawrence Livermore National Laboratory.
Abstract (Originalsprache)
DFT calculations of Sillén phases reveal high proton solubility and facile 2D diffusion within Bi–O layers. The results highlight a coupled defect chemistry between hydrogen and oxygen defects for optimized transport.
Förderung
- Hydrogen and Fuel Cell Technologies Office
- Office of Energy Efficiency and Renewable Energy
- Lawrence Livermore National Laboratory
- National Renewable Energy Laboratory
Zitieren
APA
Kang, S., Rowberg, A. J. E., Zhang, S., & Varley, J. B. (2026). Hydrogen defects in LaBi 2 O 4 X (X = Cl, Br, and I) Sillén oxyhalide phases and their impacts on ionic transport. Journal of Materials Chemistry A, 14(23), 14445-14453. https://doi.org/10.1039/d5ta09720g
Vancouver
Kang S, Rowberg AJE, Zhang S, Varley JB. Hydrogen defects in LaBi 2 O 4 X (X = Cl, Br, and I) Sillén oxyhalide phases and their impacts on ionic transport. Journal of Materials Chemistry A. 2026;14(23):14445-14453. doi:10.1039/d5ta09720g
BibTeX
@article{Kang2026,
author = {Kang, ShinYoung and Rowberg, Andrew J. E. and Zhang, Shenli and Varley, Joel B.},
title = {Hydrogen defects in LaBi 2 O 4 X (X = Cl, Br, and I) Sillén oxyhalide phases and their impacts on ionic transport},
journal = {Journal of Materials Chemistry A},
year = {2026},
volume = {14},
number = {23},
pages = {14445--14453},
doi = {10.1039/d5ta09720g}
}
EUVIMED