Short-time high-temperature oxidation behavior of nanocrystalline Ta coating at 850 °C
npj Materials Degradation · 17.05.2024 · 8 (1)
DOI: 10.1038/s41529-024-00465-7 ↗Kurz gefasst
Fachartikel in der Zeitschrift npj Materials Degradation, online erschienen am 17.05.2024. Verfasst von Yunsong Niu und 6 weiteren Autor:innen. Die Arbeit wurde bisher 12-mal zitiert (Crossref) und nennt 39 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: National Natural Science Foundation of China.
Abstract (Originalsprache)
Short-time oxidation behavior of nanocrystalline Ta coating is studied at 850 °C in comparison with that of the Ta sheet. Owing to the large PBR value and insufficient expansion space, the oxide scale on Ta sheet is dramatically cracked, delaminated and pulverized, resulting in rapid deterioration. For nanocrystalline Ta coatings with columnar structures and quantitative grain boundaries, a rapid oxygen diffusion rate causes no initial Ta 2 O 5 to form. The gap between columns provides spaces for bulk expansion, resulting in few opening cracks and delamination. Ta oxidation experiences a crystallization course from amorphous Ta oxide, leading to in situ temperature surging and thus pulverization.
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Niu, Y., Xing, L., Zhu, S., Huang, J., Chen, M., Wang, F., & Chen, Q. (2024). Short-time high-temperature oxidation behavior of nanocrystalline Ta coating at 850 °C. npj Materials Degradation, 8(1). https://doi.org/10.1038/s41529-024-00465-7
Vancouver
Niu Y, Xing L, Zhu S, Huang J, Chen M, Wang F, et al. Short-time high-temperature oxidation behavior of nanocrystalline Ta coating at 850 °C. npj Materials Degradation. 2024;8(1). doi:10.1038/s41529-024-00465-7
BibTeX
@article{Niu2024,
author = {Niu, Yunsong and Xing, Lingling and Zhu, Shenglong and Huang, Jinfeng and Chen, Minghui and Wang, Fuhui and Chen, Qiang},
title = {Short-time high-temperature oxidation behavior of nanocrystalline Ta coating at 850 °C},
journal = {npj Materials Degradation},
year = {2024},
volume = {8},
number = {1},
doi = {10.1038/s41529-024-00465-7}
}
EUVIMED