Self-Limited Reconstruction of NiFe-Based Electrocatalysts Enables Thousand-Hour Water Oxidation at Ampere-Level Current Densities

Yanbing Huang, Xuran Mao, Zongyuan Wang, Wen Guo, Jichang Liu, Fuxi Bao

ACS Sustainable Chemistry & Engineering · 10.08.2026 · 14 (31) · 14005-14016

DOI: 10.1021/acssuschemeng.6c03993 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Sustainable Chemistry & Engineering, online erschienen am 28.07.2026. Verfasst von Yanbing Huang und 5 weiteren Autor:innen. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 64 Literaturangaben. Gefördert von: National Talent Plan Project.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

NiFe-based materials are highly promising electrocatalysts for the oxygen evolution reaction (OER), but they deeply reconstruct into the low-activity γ-NiFeOOH phase in alkaline media. Herein, we propose a corrosion strategy to achieve self-limited reconstruction (SLR) of NiFe-based electrocatalysts. Ultimately, the constructed (Fe0.67Ni0.33)OOH@FeP4 selectively reconstructs into highly active β-NiFeOOH rather than the less active γ-NiFeOOH. The SLR can be described as follows: when the (Fe0.67Ni0.33)OOH@FeP4 electrocatalyst is reconstructed into the β-NiFeOOH phase, the intrinsic characteristics of the electrocatalyst itself prevent the further transformation of β-NiFeOOH into the γ-NiFeOOH phase. In situ Raman, X-ray photoelectron spectroscopy, and density functional theory (DFT) calculations suggest that the synthesized (Fe0.67Ni0.33)OOH@FeP4 reconstructs into β-NiFeOOH featuring Fe−O−Ni linkages during OER, where electron transfer from Fe to Ni through Fe−O−Ni linkages suppresses the β-NiFeOOH to γ-NiFeOOH phase transition, thereby stabilizing the β-phase. DFT calculations reveal that the (Fe0.67Ni0.33)OOH@FeP4 enhances OER kinetics by promoting the formation of the *OOH intermediate. This mechanism enables the electrocatalyst to maintain excellent durability for over 1000 h in both the OER and overall water splitting at ≥1.0 A cm−2. In an anion-exchange membrane electrolyzer, it maintains 1.5 A cm−2 at 2.25 V for 150 h, superior to many NiFe-based electrocatalysts in the literature.

Förderung

  • National Talent Plan Project

Zitieren

APA

Huang, Y., Mao, X., Wang, Z., Guo, W., Liu, J., & Bao, F. (2026). Self-Limited Reconstruction of NiFe-Based Electrocatalysts Enables Thousand-Hour Water Oxidation at Ampere-Level Current Densities. ACS Sustainable Chemistry & Engineering, 14(31), 14005-14016. https://doi.org/10.1021/acssuschemeng.6c03993

Vancouver

Huang Y, Mao X, Wang Z, Guo W, Liu J, Bao F. Self-Limited Reconstruction of NiFe-Based Electrocatalysts Enables Thousand-Hour Water Oxidation at Ampere-Level Current Densities. ACS Sustainable Chemistry & Engineering. 2026;14(31):14005-14016. doi:10.1021/acssuschemeng.6c03993

BibTeX
@article{Huang2026,
  author = {Huang, Yanbing and Mao, Xuran and Wang, Zongyuan and Guo, Wen and Liu, Jichang and Bao, Fuxi},
  title = {Self-Limited Reconstruction of NiFe-Based Electrocatalysts Enables Thousand-Hour Water Oxidation at Ampere-Level Current Densities},
  journal = {ACS Sustainable Chemistry & Engineering},
  year = {2026},
  volume = {14},
  number = {31},
  pages = {14005--14016},
  doi = {10.1021/acssuschemeng.6c03993}
}
Kostenlos starten →