Tuning the UV–Vis Light Shielding and Photocatalytic Activity of ZnO via Ag + /Fe 3+ Doping and Annealing

Yen-Ling Tsai iD, Chih-Ling Shen, Chao-Chin Su

ACS Omega · 23.06.2026 · 11 (24) · 36061-36075

DOI: 10.1021/acsomega.6c03136 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Omega, online erschienen am 09.06.2026. Verfasst von Yen-Ling Tsai und 2 weiteren Autor:innen. Beteiligte Einrichtung: Department of Cosmetic Science, Vanung University, Taoyuan 320313, Taiwan. Die Arbeit nennt 87 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

ZnO exhibits good sunscreen properties; however, its effectiveness against UVA and visible light still requires improvement. In this study, a simple chemical precipitation method combined with annealing treatment and the introduction of silver ions (Ag+) and ferric ions (Fe3+) was employed to modify the structure of ZnO particles and evaluate their effects on UV–Vis light transmittance and photocatalytic activities. ZnO, Ag+-doped ZnO, and Fe3+-doped ZnO particles were prepared by varying the molar ratios of silver nitrate or iron sulfate to zinc hydroxide, followed by annealing at 70, 200, 300, 400, and 500 °C. X-ray diffraction (XRD) and Fourier-transform infrared (FTIR) spectroscopy analyses revealed changes in the crystal structure of ZnO after annealing and Ag+/Fe3+ doping. UV–Vis spectroscopy measurements showed that both annealing temperature and metal ion doping significantly reduced light transmittance. As the annealing temperature raised and the doping concentrations of Ag+ and Fe3+ increased, the light transmittance of ZnO particles decreased accordingly. In particular, Ag+-doped ZnO particles exhibited the best shielding performance against UVA, UVB, and visible light. Photocatalytic experiments using phenol as a model degradant revealed that appropriate Ag+ and Fe3+ doping reduced the photocatalytic activity of ZnO particles. In this study, ZnO particles annealed at 500 °C, along with Ag+-doped ZnO and Fe3+-doped ZnO prepared with optimal doping amounts of 2.81 wt % Ag+ and 3.63 wt % Fe3+, respectively, exhibited the lowest photocatalytic activity.

Autor:innen und Institutionen

  • Department of Cosmetic Science, Vanung University, Taoyuan 320313, Taiwan.
  • Department of Molecular Science and Engineering, National Taipei University of Technology, Taipei 106344, Taiwan.

ORCID-Profile: Yen-Ling Tsai

Zitieren

APA

Tsai, Y. L., Shen, C. L., & Su, C. C. (2026). Tuning the UV–Vis Light Shielding and Photocatalytic Activity of ZnO via Ag + /Fe 3+ Doping and Annealing. ACS Omega, 11(24), 36061-36075. https://doi.org/10.1021/acsomega.6c03136

Vancouver

Tsai YL, Shen CL, Su CC. Tuning the UV–Vis Light Shielding and Photocatalytic Activity of ZnO via Ag + /Fe 3+ Doping and Annealing. ACS Omega. 2026;11(24):36061-36075. doi:10.1021/acsomega.6c03136

BibTeX
@article{Tsai2026,
  author = {Tsai, Yen-Ling and Shen, Chih-Ling and Su, Chao-Chin},
  title = {Tuning the UV–Vis Light Shielding and Photocatalytic Activity of ZnO via Ag + /Fe 3+ Doping and Annealing},
  journal = {ACS Omega},
  year = {2026},
  volume = {11},
  number = {24},
  pages = {36061--36075},
  doi = {10.1021/acsomega.6c03136}
}
Kostenlos starten →