Rubbery Soft Polymer Electrolyte Membrane with a Nanomatrix Channel Prepared from Natural Rubber
ACS Omega · 06.05.2025 · 10 (17) · 17576-17583
DOI: 10.1021/acsomega.4c11363 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Omega, online erschienen am 23.04.2025. Verfasst von Yoshimasa Yamamoto und 1 weiteren Autor:innen. Beteiligte Einrichtung: Department of Chemical Science and Engineering, National Institute of Technology, Tokyo College, 1220-2 Kunugida, Hachioji, Tokyo 193-0997, Japan. Die Arbeit wurde bisher 4-mal zitiert (Crossref) und nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: Japan Society for the Promotion of Science.
Abstract (Originalsprache)
Rubbery soft polymer electrolyte membranes (PEMs) prepared from naturally occurring products are in high demand for the fabrication of flexible fuel cells as a multipurpose energy source to achieve a carbon-neutral society. This work describes the preparation of a rubbery soft PEM from deproteinized natural rubber (DPNR) by grafting-copolymerizing ethyl p-styrenesulfonate (SSEt) onto the surface of rubber particles in the latex stage, followed by hydrolysis with NaOH and cast film formation to construct a nanomatrix channel. The resulting rubbery soft PEM, a graft copolymer of DPNR and poly(p-styrenesulfonic acid) (DPNR-graft-PSS), is characterized by 1H NMR spectroscopy, transmission electron microscopy (TEM), impedance analysis, and tensile testing. The hydrophobic rubber particles with a diameter of about 1 μm are well dispersed in the continuous nanochannel of hydrophilic poly(p-styrenesulfonic acid) with a thickness of about 10 nm that possesses a high proton conductivity, owing to an efficient proton transportation, which is beneficial for polymer electrolyte fuel cells. σ* is the proton conductivity per unit equivalent of sulfonic acid, which is distinguished from the proton conductivity, σ. The value of σ* for the DPNR-graft-PSS prepared with 1.0 mol/kg-rubber of SSEt is 2.6 (S/cm)/meq, which is approximately 1.4 times higher than that of the perfluorosulfonic acid membrane Nafion117, whereas its σ is lower. The apparent activation energy of DPNR-graft-PSS (3.2 kJ/mol) is lower than that of Nafion117, and its stress at break (6.9 MPa) is higher than that of DPNR. The high σ*, low apparent activation energy, and outstanding tensile strength of DPNR-graft-PSS can be attributed to the formation of the nanomatrix channel.
Autor:innen und Institutionen
- Department of Chemical Science and Engineering, National Institute of Technology, Tokyo College, 1220-2 Kunugida, Hachioji, Tokyo 193-0997, Japan.
- Department of Materials Science and Bioengineering, Nagaoka University of Technology, 1603-1, Kamitomioka-cho, Nagaoka, Niigata 940-2188, Japan.
ORCID-Profile: Yoshimasa Yamamoto, Seiichi Kawahara
Förderung
- Japan Society for the Promotion of Science
Zitieren
APA
Yamamoto, Y., & Kawahara, S. (2025). Rubbery Soft Polymer Electrolyte Membrane with a Nanomatrix Channel Prepared from Natural Rubber. ACS Omega, 10(17), 17576-17583. https://doi.org/10.1021/acsomega.4c11363
Vancouver
Yamamoto Y, Kawahara S. Rubbery Soft Polymer Electrolyte Membrane with a Nanomatrix Channel Prepared from Natural Rubber. ACS Omega. 2025;10(17):17576-17583. doi:10.1021/acsomega.4c11363
BibTeX
@article{Yamamoto2025,
author = {Yamamoto, Yoshimasa and Kawahara, Seiichi},
title = {Rubbery Soft Polymer Electrolyte Membrane with a Nanomatrix Channel Prepared from Natural Rubber},
journal = {ACS Omega},
year = {2025},
volume = {10},
number = {17},
pages = {17576--17583},
doi = {10.1021/acsomega.4c11363}
}
EUVIMED