Fachartikel in der Zeitschrift ACS ES&T Engineering, online erschienen am 06.08.2026. Verfasst von Biraj Saha und 3 weiteren Autor:innen. Die Arbeit wurde bisher 1-mal zitiert (Crossref) und nennt 92 Literaturangaben. Gefördert von: Environmental Research and Education Foundation, North Dakota State University, National Science Foundation.
Abstract (Originalsprache)
Plastics entering composting systems are frequently found as fragments in finished compost, yet the mechanisms controlling their degradation and persistence remain unclear. In this study, food waste amended with virgin, 30-day UV-weathered, and 30-day sunlight-weathered polyethylene (PE) and poly(methyl methacrylate) (PMMA) microbeads was treated under aerobic and hyperthermophilic composting conditions. PE showed increased surface oxidation after both composting conditions, with the carbonyl index increasing from 3.6–16.6 in virgin to 12.2–25.1 in UV-weathered and 15.0–21.3 in sunlight-weathered beads. This oxidation corresponded with a decreased C/O ratio due to the formation of carbonyl and ester/carboxyl groups. Composting increased crack density on PE surfaces without altering molecular weight, indicating surface-limited degradation. In contrast, PMMA showed a 44–71% decrease in molecular weight after weathering, but no additional molecular weight reduction occurred during composting of weathered PMMA beads. After exposure to both composting conditions, PMMA showed increased thermal stability, whereas PE showed decreased thermal stability. Degradation rates were 6.2–19.5 μm yr–1 for PE and 5.9–33.9 μm yr–1 for PMMA, with estimated degradation times of 8.6–26.9 and 5.8–41.9 years, respectively. A field study showed that surface oxidation and crack density of PE, PP, PS, and PET correlated with compost maturity, likely due to prolonged exposure to dynamic composting conditions. These findings reveal plastic degradation pathways in compost and enable the prediction of their long-term environmental fate.
Förderung
- Environmental Research and Education Foundation
- North Dakota State University
- National Science Foundation
Zitieren
APA
Saha, B., Ateia, M., Eagan, J. M., & Iskander, S. M. (2026). Surface-Limited Chemical and Physical Alteration of Plastics during Composting: An In-Depth Field- and Lab-Scale Study. ACS ES&T Engineering, 6(9), 2438-2448. https://doi.org/10.1021/acsestengg.6c00349
Vancouver
Saha B, Ateia M, Eagan JM, Iskander SM. Surface-Limited Chemical and Physical Alteration of Plastics during Composting: An In-Depth Field- and Lab-Scale Study. ACS ES&T Engineering. 2026;6(9):2438-2448. doi:10.1021/acsestengg.6c00349
BibTeX
@article{Saha2026,
author = {Saha, Biraj and Ateia, Mohamed and Eagan, James M. and Iskander, Syeed Md},
title = {Surface-Limited Chemical and Physical Alteration of Plastics during Composting: An In-Depth Field- and Lab-Scale Study},
journal = {ACS ES&T Engineering},
year = {2026},
volume = {6},
number = {9},
pages = {2438--2448},
doi = {10.1021/acsestengg.6c00349}
}
EUVIMED