Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners
ACS Applied Polymer Materials · 17.11.2026
DOI: 10.1021/acsapm.6c03876 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Polymer Materials, online erschienen am 17.11.2026. Verfasst von Mohammadjavad Haji Rezaei und 6 weiteren Autor:innen. Die Arbeit nennt 33 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Pipeline and Hazardous Materials Safety Administration.
Abstract (Originalsprache)
Polymeric materials are increasingly used in natural gas infrastructure, yet their long-term reliability under realistic service conditions remains poorly characterized, particularly in the presence of potential reactive contaminants. In this work, we investigate the aging behavior of high-density polyethylene (HDPE), nylon-6/6 polyamide (PA), and poly(vinylidene fluoride) (PVDF) exposed to a natural gas mixture containing 0.5% oxygen as a model reactive contaminant. Using dynamic mechanical analysis (DMA), time–temperature superposition (TTS), and Fourier-transform infrared spectroscopy (FTIR), we characterize the evolution of mechanical properties, viscoelastic relaxation dynamics, and chemical structure under accelerated aging conditions with elevated temperature and pressure. While conventional mechanical properties provide ambiguous and often noisy metrics, we observe a pronounced reduction in the activation energy Ea associated with segmental relaxation across all polymers, indicating accelerated molecular dynamics. The presence of oxygen significantly enhances this effect, particularly at early aging times. We classify the aging response based on whether activation energy Ea recovers after the polymer is removed from the gas environment. For HDPE, PVDF, and PA samples aged at room temperature, the decrease in Ea recovers almost entirely once the polymers are removed from the natural gas environment, consistent with physical absorption. By contrast, PA samples aged at 90 °C exhibit only partial recovery of mechanical properties and persistent FTIR features, indicating chemical changes induced by the oxygenated environment. These results demonstrate that viscoelastic measurements can distinguish between reversible and irreversible degradation processes that may not be detected by conventional measurements.
Förderung
- Pipeline and Hazardous Materials Safety Administration
Zitieren
APA
Rezaei, M. H., Ghosh, D., Alkhoury, K., Lyakhovych, Z., Mathiowitz, E., Srivastava, V., & Poling-Skutvik, R. (2026). Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners. ACS Applied Polymer Materials. https://doi.org/10.1021/acsapm.6c03876
Vancouver
Rezaei MH, Ghosh D, Alkhoury K, Lyakhovych Z, Mathiowitz E, Srivastava V, et al. Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners. ACS Applied Polymer Materials. 2026. doi:10.1021/acsapm.6c03876
BibTeX
@article{Rezaei2026,
author = {Rezaei, Mohammadjavad Haji and Ghosh, Deepro and Alkhoury, Keven and Lyakhovych, Zakhar and Mathiowitz, Edith and Srivastava, Vikas and Poling-Skutvik, Ryan},
title = {Distinguishing Reversible Plasticization and Irreversible Degradation in Polymeric Liners},
journal = {ACS Applied Polymer Materials},
year = {2026},
doi = {10.1021/acsapm.6c03876}
}
EUVIMED