Hydroalcoholic-Induced Multiscale Reorganization of Sulfonated Poly(ether ether ketone) (sPEEK) Membranes
ACS Applied Polymer Materials · 14.08.2026 · 8 (15) · 13227-13237
DOI: 10.1021/acsapm.6c02345 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Polymer Materials, online erschienen am 27.07.2026. Verfasst von Maxime Gondrexon und 5 weiteren Autor:innen. Die Arbeit nennt 50 Literaturangaben.
Abstract (Originalsprache)
Next-generation proton exchange membrane fuel cells (PEMFCs) require membranes that combine high proton conductivity, low gas permeability, and mechanical robustness under harsh conditions, yet many commercial options struggle to meet these criteria simultaneously. Sulfonated poly(ether ether ketone) (sPEEK) is a promising nonfluorinated alternative. Hydrothermal (HT) treatment can control sPEEK nanostructure and enhance functional properties, but intrinsic morphological variations lead to markedly different responses, including membrane failure in liquid water at elevated temperature, showing that HT alone is not universally effective. Here, we demonstrate that hydroalcoholic (HA) treatment provides a robust and broadly applicable approach to control sPEEK nanostructure and optimize functional performance. HA pretreatment enhances proton conductivity and water uptake while allowing the membranes to withstand liquid water at 80 °C under the investigated conditions. Small-angle X-ray and neutron scattering (SAXS and SANS) reveal well-connected ionic channels, nanoscale swelling, and reorganized mesoscale interbundle regions. Comparison of commercial sPEEK membranes indicates that HA specifically drives structural rearrangements in interbundle regions, which appear to influence ionic channel connectivity and mesoscale organization, thereby strongly affecting the membrane macroscopic properties. These findings highlight the pivotal role of solvent–polymer interactions at multiple length scales and provide practical guidelines for selecting HA composition and processing conditions. HA thus emerges as a scalable and broadly applicable strategy to simultaneously optimize proton transport through solvent-induced mesoscale reorganization of sPEEK membranes for demanding PEMFC applications. Owing to its simplicity, this treatment can be readily implemented either inline during membrane fabrication or as a post-treatment step before membrane-electrode assembly (MEA).
Zitieren
APA
Gondrexon, M., Gonon, L., Mareau, V. H., Porcar, L., Pouget, S., & Mendil-Jakani, H. (2026). Hydroalcoholic-Induced Multiscale Reorganization of Sulfonated Poly(ether ether ketone) (sPEEK) Membranes. ACS Applied Polymer Materials, 8(15), 13227-13237. https://doi.org/10.1021/acsapm.6c02345
Vancouver
Gondrexon M, Gonon L, Mareau VH, Porcar L, Pouget S, Mendil-Jakani H. Hydroalcoholic-Induced Multiscale Reorganization of Sulfonated Poly(ether ether ketone) (sPEEK) Membranes. ACS Applied Polymer Materials. 2026;8(15):13227-13237. doi:10.1021/acsapm.6c02345
BibTeX
@article{Gondrexon2026,
author = {Gondrexon, Maxime and Gonon, Laurent and Mareau, Vincent H. and Porcar, Lionel and Pouget, Stéphanie and Mendil-Jakani, Hakima},
title = {Hydroalcoholic-Induced Multiscale Reorganization of Sulfonated Poly(ether ether ketone) (sPEEK) Membranes},
journal = {ACS Applied Polymer Materials},
year = {2026},
volume = {8},
number = {15},
pages = {13227--13237},
doi = {10.1021/acsapm.6c02345}
}
EUVIMED