Sn@C Composite with an Ultra-high Initial Coulombic Efficiency via Interfacial Engineering for Sodium-Ion Battery Anodes
ACS Applied Materials & Interfaces · 11.11.2026 · 18 (44) · 60777-60789
DOI: 10.1021/acsami.6c16359 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 29.10.2026. Verfasst von Xi-Yu Zhang und 6 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Special Functional Materials and Devices of Ministry of Education, College of Chemistry and Chemical Engineering, Lanzhou Universit…. Die Arbeit nennt 54 Literaturangaben. Gefördert von: Fundamental Research Funds for the Central Universities, Key Research and Development Program of Jiangxi Province.
Abstract (Originalsprache)
Tin (Sn)-based anodes are attractive candidates for sodium-ion batteries due to their high theoretical capacity and low operating potential. However, their practical viability is severely constrained by drastic volume changes, unstable solid–electrolyte interphase (SEI) formation, and intrinsically low initial Coulombic efficiency (ICE). Herein, an interfacial regulation strategy to enhance the ICE and cycling stability of Sn-based anodes is proposed. That is, we construct Sn-MOF-derived Sn@C composites with submicron Sn particles uniformly confined in a conductive carbon matrix via hydrothermal synthesis and subsequent pyrolysis. This architecture yields an exceptional ICE of 96.4% (725/752 mA h g–1 at 0.1 A g–1), far surpassing that of commercial Sn powder (77.9%). Mechanistic investigations reveal a reversible stepwise alloying pathway from Sn to Na9Sn4 and subsequently to Na15Sn4, while the carbon matrix promotes a thin, uniform NaF-rich SEI that curbs electrolyte decomposition and Na+ loss. In situ EIS-DRT analysis further corroborates the progressive reduction of interfacial resistances during sodiation–desodiation. As a result, the anode sustains 378 mA h g–1 after 500 cycles at 1 A g–1. A Sn@C-900∥Na3V2(PO4)3 full cell can deliver an energy density of 188 W h kg–1 and retain 107 mA h g–1 over 400 cycles, underscoring the practical feasibility of this high-ICE Sn@C anode.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Key Laboratory of Special Functional Materials and Devices of Ministry of Education, College of Chemistry and Chemical Engineering, Lanzhou University, Lanzhou730000, P.R. China.
ORCID-Profile: Yong-Qing Zhao
Förderung
- Fundamental Research Funds for the Central Universities
- Key Research and Development Program of Jiangxi Province
Zitieren
APA
Zhang, X. Y., Zhang, Y. H., Wang, T. X., Wang, W. J., Zhang, Y. S., Hu, J. H., & Zhao, Y. Q. (2026). Sn@C Composite with an Ultra-high Initial Coulombic Efficiency via Interfacial Engineering for Sodium-Ion Battery Anodes. ACS Applied Materials & Interfaces, 18(44), 60777-60789. https://doi.org/10.1021/acsami.6c16359
Vancouver
Zhang XY, Zhang YH, Wang TX, Wang WJ, Zhang YS, Hu JH, et al. Sn@C Composite with an Ultra-high Initial Coulombic Efficiency via Interfacial Engineering for Sodium-Ion Battery Anodes. ACS Applied Materials & Interfaces. 2026;18(44):60777-60789. doi:10.1021/acsami.6c16359
BibTeX
@article{Zhang2026,
author = {Zhang, Xi-Yu and Zhang, Yao-He and Wang, Tian-Xiang and Wang, Wei-Jie and Zhang, Yu-Sheng and Hu, Jing-Hang and Zhao, Yong-Qing},
title = {Sn@C Composite with an Ultra-high Initial Coulombic Efficiency via Interfacial Engineering for Sodium-Ion Battery Anodes},
journal = {ACS Applied Materials & Interfaces},
year = {2026},
volume = {18},
number = {44},
pages = {60777--60789},
doi = {10.1021/acsami.6c16359}
}