Wettability-Gradient Interphase for Reconciling Water Shielding with Zincate Transport in Alkaline Zn–Ni Batteries

Mengyue Liu, Hao Tian, Guisheng Guo, Yong Gao, Sajid Ullah, Zhenwen Yu, Zhuang Jiang, Kun Chang iD

ACS Applied Materials & Interfaces · 28.10.2026 · 18 (42) · 58391-58402

DOI: 10.1021/acsami.6c15271 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 19.10.2026. Verfasst von Mengyue Liu und 7 weiteren Autor:innen. Beteiligte Einrichtung: College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing210016, PR China. Die Arbeit nennt 49 Literaturangaben. Gefördert von: National Natural Science Foundation of China (NSFC).

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Artificial interfacial layers on Zn anodes are a promising route for stabilizing alkaline Zn–Ni batteries, but their practical effectiveness is often limited by a trade-off between suppressing water-induced parasitic reactions and maintaining rapid Zn-containing species transport. Herein, a hydrophobic–hydrophilic gradient composite layer is developed on a Zn substrate through sequential perfluorooctyltrichlorosilane (PFOTS) modification followed by crosslinked polyvinyl alcohol (PVA) coating. This gradient interphase couples a buried hydrophobic PFOTS layer with an outer hydrophilic PVA layer, thereby balancing water shielding, electrolyte affinity, mechanical compliance, and Zn-containing species transport at the Zn/electrolyte interface. As a result, the symmetric cell based on PFOTS/PVA-modified Zn (ZP) delivers stable cycling for 1200 h at 1 mA cm–2 and 1 mAh cm–2. When coupled with a Ni(OH)2-based cathode, the resulting alkaline Zn–Ni full cell exhibits an output voltage of ≈1.77 V, retains 93.2% of its capacity after resting for 48 h, sustains stable operation for more than 1100 h at 1 C, and maintains durable cycling over 1500 cycles at 2 C. This work demonstrates that wettability-gradient interfacial engineering can reconcile water regulation, Zn-containing species transport, and mechanical compliance for durable alkaline Zn anodes.

Schlagwörter

Stichwörter der Autor:innen

PFOTSZn anodealkaline Zn–Ni batterieshydrophobic–hydrophilic gradientinterfacial microenvironment

Autor:innen und Institutionen

  • College of Materials Science and Technology, Nanjing University of Aeronautics and Astronautics, Nanjing210016, PR China.

ORCID-Profile: Kun Chang

Förderung

  • National Natural Science Foundation of China (NSFC)

Zitieren

APA

Liu, M., Tian, H., Guo, G., Gao, Y., Ullah, S., Yu, Z., Jiang, Z., & Chang, K. (2026). Wettability-Gradient Interphase for Reconciling Water Shielding with Zincate Transport in Alkaline Zn–Ni Batteries. ACS Applied Materials & Interfaces, 18(42), 58391-58402. https://doi.org/10.1021/acsami.6c15271

Vancouver

Liu M, Tian H, Guo G, Gao Y, Ullah S, Yu Z, et al. Wettability-Gradient Interphase for Reconciling Water Shielding with Zincate Transport in Alkaline Zn–Ni Batteries. ACS Applied Materials & Interfaces. 2026;18(42):58391-58402. doi:10.1021/acsami.6c15271

BibTeX
@article{Liu2026,
  author = {Liu, Mengyue and Tian, Hao and Guo, Guisheng and Gao, Yong and Ullah, Sajid and Yu, Zhenwen and Jiang, Zhuang and Chang, Kun},
  title = {Wettability-Gradient Interphase for Reconciling Water Shielding with Zincate Transport in Alkaline Zn–Ni Batteries},
  journal = {ACS Applied Materials & Interfaces},
  year = {2026},
  volume = {18},
  number = {42},
  pages = {58391--58402},
  doi = {10.1021/acsami.6c15271}
}
Kostenlos starten →