EUVIMEDEUVIMED entdecken
Crossref

In Situ Atomic Arrangement and Defect Engineering of Li-Rich Cathodes for Interface Stabilization

Yueying Liu, Mengke Zhang, Shuli Zheng, Binbin Yan, Yu Shi, Jiahui Xu, Lang Qiu, Xiaodong Guo iD

ACS Applied Materials & Interfaces · 22.04.2026 · 18 (15) · 21913-21923

DOI: 10.1021/acsami.5c25069 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 09.04.2026. Verfasst von Yueying Liu und 7 weiteren Autor:innen. Beteiligte Einrichtung: School of Chemical Engineering, Sichuan University, Chengdu 610065, P. R. China. Die Arbeit wurde bisher 2-mal zitiert (Crossref) und nennt 65 Literaturangaben. Gefördert von: Science and Technology Department of Sichuan Province, National Natural Science Foundation of China, National Science and Technology Major Project.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Coming research trends will move toward high-energy-density Li-rich manganese layered (LMR) cathodes (>900 Wh kg-1). Nevertheless, their practical implementation is severely impeded by irreversible lattice oxygen release, progressive structural deterioration, pronounced capacity, and voltage decay. A critical unresolved issue arises from the absence of an effective atomic-scale design principle capable of stabilizing the interfacial structure and suppressing the layer-to-rock salt transformation, an instability pathway that is further aggravated in high-Ni LMR compositions. In this work, we establish an in situ atomic-level regulation strategy through La3+/W6+ codoping, which induces the formation of an interface-disordered phase while preserving the integrity of the layered framework. This strategy provides a direct resolution to this long-standing structural challenge by enabling controlled oxygen-vacancy generation and localized cation rearrangement at the near-surface region, thereby effectively suppressing detrimental phase transitions during electrochemical cycling and simultaneously enhancing Li+ transport kinetics. The introduction of robust La-O and W-O bonds further reinforces the interfacial oxygen framework and markedly improves thermal stability. As a consequence, the modified cathode demonstrates substantially enhanced electrochemical durability. Compared with the original sample, the capacity retention rate of LW-3 is 80.25%, which is significantly better than that of LMR (66.26%). Moreover, the results substantiate that high-Ni LMR compositions possess an intrinsic propensity toward layered-to-rock-salt transformation, which profoundly compromises structural and electrochemical stability. This work strengthens the structural integrity and mechanical resilience of LMR cathodes and offers a responsible strategy toward realizing high-energy, long-life Li-rich layered oxides suitable for next-generation energy storage technologies.

Schlagwörter

Stichwörter der Autor:innen

Li-rich cathodescycling stabilityinterface-disordered phaseoxygen vacanciesvoltage decay

Autor:innen und Institutionen

  • School of Chemical Engineering, Sichuan University, Chengdu 610065, P. R. China.

ORCID-Profile: Xiaodong Guo

Förderung

  • Science and Technology Department of Sichuan Province
  • National Natural Science Foundation of China
  • National Science and Technology Major Project

Zitieren

APA

Liu, Y., Zhang, M., Zheng, S., Yan, B., Shi, Y., Xu, J., Qiu, L., & Guo, X. (2026). In Situ Atomic Arrangement and Defect Engineering of Li-Rich Cathodes for Interface Stabilization. ACS Applied Materials & Interfaces, 18(15), 21913-21923. https://doi.org/10.1021/acsami.5c25069

Vancouver

Liu Y, Zhang M, Zheng S, Yan B, Shi Y, Xu J, et al. In Situ Atomic Arrangement and Defect Engineering of Li-Rich Cathodes for Interface Stabilization. ACS Applied Materials & Interfaces. 2026;18(15):21913-21923. doi:10.1021/acsami.5c25069

BibTeX
@article{Liu2026,
  author = {Liu, Yueying and Zhang, Mengke and Zheng, Shuli and Yan, Binbin and Shi, Yu and Xu, Jiahui and Qiu, Lang and Guo, Xiaodong},
  title = {In Situ Atomic Arrangement and Defect Engineering of Li-Rich Cathodes for Interface Stabilization},
  journal = {ACS Applied Materials & Interfaces},
  year = {2026},
  volume = {18},
  number = {15},
  pages = {21913--21923},
  doi = {10.1021/acsami.5c25069}
}
Kostenlos starten →