Degradation of PGM and PGM-free Coatings on PEMWE Porous Transport Layers
ACS Applied Materials & Interfaces · 26.03.2025 · 17 (12) · 19070-19085
DOI: 10.1021/acsami.4c22455 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 11.03.2025. Verfasst von Lukas Stein und 5 weiteren Autor:innen. Beteiligte Einrichtung: Leibniz University Hannover, Institute of Electric Power Systems, Appelstraße 9A, Hannover 30167, Germany. Die Arbeit wurde bisher 44-mal zitiert (Crossref) und nennt 45 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY 4.0). Gefördert von: Bundesministerium für Bildung und Forschung, Niedersächsisches Ministerium für Wissenschaft und Kultur.
Abstract (Originalsprache)
High Resolution Image Download MS PowerPoint Slide A good and long-term stable electrical contact between the porous anode transport layer (PTL) and the adjacent catalyst layer is essential for efficient polymer electrolyte membrane water electrolyzers. This study describes the extensive comparison of seven titanium passivation-protecting coatings using short- and long-term measurements for at least 2000 h. The measurements are supported by before and after scanning electron microscope investigations of cross sections, energy-dispersive X-ray spectroscopy, X-ray diffractometry of the coatings, contact resistance measurements, and ex situ rapid aging tests. Overall, iridium and platinum PTL coatings offer outstanding contact and excellent corrosion protection. Compared to the uncoated reference sample, platinum shows a 93% reduction in the overall degradation rate to 7 μV h –1 (at a current density of 3 A cm –2 ) over 5000 h and even reduces ohmic overvoltages over time in the first 2000 h. Interestingly, the interface to the flow field does not appear to be influenced by precious metal coatings and, hence, does not need to be coated. In contrast, niobium and titanium nitride PTL coatings under investigation do not provide an improvement compared to the uncoated reference but show dissolution and oxidation phenomena, respectively. Titanium hydride produced by hydrochloric acid improves the electrical contact and reduces degradation by 49% overall and 62% in terms of ohmic overvoltages compared to the uncoated reference. It also shows a saturation behavior in degradation with a stable rate of 23 μV h –1 in the second 1000 h of the measurement. Ex situ rapid aging tests additionally support the main trends. For all surface treatments, more detailed information about the occurring aging mechanisms and reversible overvoltages is obtained by separating the degradation rate into partial rates of the overvoltage mechanisms.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Leibniz University Hannover, Institute of Electric Power Systems, Appelstraße 9A, Hannover 30167, Germany.
- Institute for Solar Energy Research Hamelin (ISFH), Am Ohrberg 1, Emmerthal 31860, Germany.
ORCID-Profile: Lukas Stein
Förderung
- Bundesministerium für Bildung und Forschung
- Niedersächsisches Ministerium für Wissenschaft und Kultur
Zitieren
APA
Stein, L., Dittrich, A., Walter, D. C., Trinke, P., Bensmann, B., & Hanke-Rauschenbach, R. (2025). Degradation of PGM and PGM-free Coatings on PEMWE Porous Transport Layers. ACS Applied Materials & Interfaces, 17(12), 19070-19085. https://doi.org/10.1021/acsami.4c22455
Vancouver
Stein L, Dittrich A, Walter DC, Trinke P, Bensmann B, Hanke-Rauschenbach R. Degradation of PGM and PGM-free Coatings on PEMWE Porous Transport Layers. ACS Applied Materials & Interfaces. 2025;17(12):19070-19085. doi:10.1021/acsami.4c22455
BibTeX
@article{Stein2025,
author = {Stein, Lukas and Dittrich, Arne and Walter, Dominic C and Trinke, Patrick and Bensmann, Boris and Hanke-Rauschenbach, Richard},
title = {Degradation of PGM and PGM-free Coatings on PEMWE Porous Transport Layers},
journal = {ACS Applied Materials & Interfaces},
year = {2025},
volume = {17},
number = {12},
pages = {19070--19085},
doi = {10.1021/acsami.4c22455}
}
EUVIMED