Electrical Conductivity Characteristic of Polyimide under Long-Term Combined Electron Irradiation and Thermal Cycle in Vacuum
ACS Applied Materials & Interfaces · 28.08.2024 · 16 (34) · 45598-45605
DOI: 10.1021/acsami.4c11229 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 15.08.2024. Verfasst von Bingying Chen und 6 weiteren Autor:innen. Beteiligte Einrichtung: State Key Laboratory of Alternate Electrical Power System with Renewable Energy Sources and the Beijing Key Laboratory of High Voltage and EMC, North…. Die Arbeit wurde bisher 5-mal zitiert (Crossref) und nennt 41 Literaturangaben. Gefördert von: National Natural Science Foundation of China.
Abstract (Originalsprache)
During long-term operation, low-earth-orbit spacecraft are exposed to a severe environment of electron irradiation and thermal cycle. This affects the electric properties of polyimide, an essential insulation material for spacecraft electrical transmission equipment, particularly the conductivity characteristic. Therefore, this paper investigates the conductivity and its evolution of polyimide after the combination of 20 keV, 8 nA/cm2 electron irradiation, and 243-343 K, 5 K/min thermal cycle in a vacuum environment for 432 h. The results show that the conductivity increases by about 2 orders of magnitude over 432 h, with the threshold field for electric-field-dependent conductivity decreasing. The conductivity growth rate varies, rising during the first 192 h, then increasing in the midelectric field, and decreasing in the high electric field regions. The thermally stimulated depolarization current method demonstrates that increases in γ, β1, and β2 trap densities, associated with enhanced motility of end groups, diamines, and dianhydrides after long-chain breaks, lead to higher conductivity and growth rate. Additionally, increases in β3 and α trap densities, related to increased C═O bonds and free radicals, reduce the threshold field and the conductivity growth rate in the range of 57.0-100.0 kV/mm after 192 h. These findings provide a reference for the performance evaluation and enhancement of spacecraft polyimide materials.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- State Key Laboratory of Alternate Electrical Power System with Renewable Energy Sources and the Beijing Key Laboratory of High Voltage and EMC, North China Electric Power University, Beijing 102206, China.
ORCID-Profile: Bingying Chen, Geng Chen
Förderung
- National Natural Science Foundation of China
Zitieren
APA
Chen, B., Chen, G., Zhang, X., Zhang, W., Tu, Y., Wang, C., & Zheng, Z. (2024). Electrical Conductivity Characteristic of Polyimide under Long-Term Combined Electron Irradiation and Thermal Cycle in Vacuum. ACS Applied Materials & Interfaces, 16(34), 45598-45605. https://doi.org/10.1021/acsami.4c11229
Vancouver
Chen B, Chen G, Zhang X, Zhang W, Tu Y, Wang C, et al. Electrical Conductivity Characteristic of Polyimide under Long-Term Combined Electron Irradiation and Thermal Cycle in Vacuum. ACS Applied Materials & Interfaces. 2024;16(34):45598-45605. doi:10.1021/acsami.4c11229
BibTeX
@article{Chen2024,
author = {Chen, Bingying and Chen, Geng and Zhang, Xintong and Zhang, Wenjia and Tu, Youping and Wang, Cong and Zheng, Zhong},
title = {Electrical Conductivity Characteristic of Polyimide under Long-Term Combined Electron Irradiation and Thermal Cycle in Vacuum},
journal = {ACS Applied Materials & Interfaces},
year = {2024},
volume = {16},
number = {34},
pages = {45598--45605},
doi = {10.1021/acsami.4c11229}
}
EUVIMED