EUVIMEDEUVIMED entdecken
Crossref

Fluorine-Rich Electrolyte Additive for Achieving Dendrite-Free Lithium Anodes at Low Temperatures

Yan Wang, Longtao Ren, Qiaoli Zhang, Abdul Hameed Pato, Jun Liu, Xiwen Lu, Wen Liu iD

ACS Applied Materials & Interfaces · 11.09.2024 · 16 (36) · 47674-47682

DOI: 10.1021/acsami.4c10028 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 30.08.2024. Verfasst von Yan Wang und 6 weiteren Autor:innen. Beteiligte Einrichtung: College of Chemistry, State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China. Die Arbeit wurde bisher 13-mal zitiert (Crossref) und nennt 40 Literaturangaben. Gefördert von: Beijing University of Chemical Technology, Natural Science Foundation of Beijing Municipality, China Three Gorges Corporation.

AbstractSchlagwörterBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

The practical application of lithium metal anodes is significantly impeded by poor interfacial stability and uncontrolled dendrite growth. Herein, we introduce methyl trifluoroacetate (MTFA), a low-melting-point small molecule, as an electrolyte additive in an ether-based electrolyte. This additive facilitates the formation of an in situ composite solid electrolyte interphase (SEI) layer that is rich in LiF and features an ester-based flexible matrix. The resulting composite layer exhibits high ionic conductivity and mechanical stability, effectively regulating the lithium deposition behavior over a broad temperature range and inhibiting dendrite formation. Based on MTFA, the Li||Li symmetrical cell achieves a lifespan exceeding 5000 h at room temperature and 800 h at -20 °C, both with ultralow overpotential and exceptional cycling stability. In Li||LiFePO4 full cells with a high-area loading (10.52 mg cm-2) and an N/P ratio of 1.68, an average capacity decay of merely 0.096% per cycle is observed over 200 cycles. Even at -20 °C, the Li||LiFePO4 cell shows a CE of over 99% and maintains stable cycling performance. This work provides an innovative approach for optimizing lithium metal anode interfaces and enhancing low-temperature operation capabilities through the use of electrolyte additives.

Schlagwörter

Stichwörter der Autor:innen

dendrite freeelectrolyte additiveslithium metal anodelow temperaturesolid electrolyte interphase

Autor:innen und Institutionen

  • College of Chemistry, State Key Laboratory of Chemical Resource Engineering, Beijing University of Chemical Technology, Beijing 100029, China.

ORCID-Profile: Wen Liu

Förderung

  • Beijing University of Chemical Technology
  • Natural Science Foundation of Beijing Municipality
  • China Three Gorges Corporation
  • National Natural Science Foundation of China

Zitieren

APA

Wang, Y., Ren, L., Zhang, Q., Pato, A. H., Liu, J., Lu, X., & Liu, W. (2024). Fluorine-Rich Electrolyte Additive for Achieving Dendrite-Free Lithium Anodes at Low Temperatures. ACS Applied Materials & Interfaces, 16(36), 47674-47682. https://doi.org/10.1021/acsami.4c10028

Vancouver

Wang Y, Ren L, Zhang Q, Pato AH, Liu J, Lu X, et al. Fluorine-Rich Electrolyte Additive for Achieving Dendrite-Free Lithium Anodes at Low Temperatures. ACS Applied Materials & Interfaces. 2024;16(36):47674-47682. doi:10.1021/acsami.4c10028

BibTeX
@article{Wang2024,
  author = {Wang, Yan and Ren, Longtao and Zhang, Qiaoli and Pato, Abdul Hameed and Liu, Jun and Lu, Xiwen and Liu, Wen},
  title = {Fluorine-Rich Electrolyte Additive for Achieving Dendrite-Free Lithium Anodes at Low Temperatures},
  journal = {ACS Applied Materials & Interfaces},
  year = {2024},
  volume = {16},
  number = {36},
  pages = {47674--47682},
  doi = {10.1021/acsami.4c10028}
}
Kostenlos starten →