Tuning Ceramic Surface to Minimize the Ionic Resistance at the Interface between PEO- and LATP-Based Ceramic Electrolyte
ACS Applied Materials & Interfaces · 28.08.2024 · 16 (34) · 45713-45723
DOI: 10.1021/acsami.4c08882 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 13.08.2024. Verfasst von Léa R Mangani und 4 weiteren Autor:innen. Beteiligte Einrichtung: Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, Grenoble INP, LEPMI, Grenoble 38000, France. Die Arbeit wurde bisher 8-mal zitiert (Crossref) und nennt 59 Literaturangaben. Gefördert von: Agence de la transition ?cologique, Association Nationale de la Recherche et de la Technologie.
Abstract (Originalsprache)
New battery technologies are currently under development, and among them, all-solid-state batteries should deliver better electrochemical performance and enhanced safety. Composite solid electrolytes, combining a solid polymer electrolyte (SPE) and a ceramic electrolyte (CE), should then provide high ionic conductivity coupled to high mechanical stability. To date, this synergy has not yet been reached due to the complexity of the Li-ion transport within the hybrid solid electrolyte, especially at the SPE/CE interface currently considered the limiting step. Yet, there is no proper kinetic model to elucidate the parameters influencing this interfacial barrier. The limited understanding of the SPE/CE interface can be partly explained by scattered SPE/CE interface resistances reported in the literature as well as the lack of systematic studies. Herein, we propose a systematic study of the effect on the SPE/CE interfacial resistance of chemical and thermal treatments of a model LATP-based ceramic based on a methodology relying on electrochemical impedance spectroscopy (EIS) and X-ray photoemission spectroscopy (XPS). The results provide different levers for the optimization of this interface and valuable insights into experimental precautions needed to obtain more reproducible results.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Univ. Grenoble Alpes, Univ. Savoie Mont Blanc, CNRS, Grenoble INP, LEPMI, Grenoble 38000, France.
- Université Grenoble Alpes, CEA, LITEN, DTNM, Grenoble 38000, France.
- SAFT, Direction de la Recherche, 111 Boulevard Alfred Daney, Bordeaux F-33000, France.
ORCID-Profile: Léa R Mangani, Didier Devaux, Anass Benayad, Renaud Bouchet
Förderung
- Agence de la transition ?cologique
- Association Nationale de la Recherche et de la Technologie
Zitieren
APA
Mangani, L. R., Devaux, D., Benayad, A., Jordy, C., & Bouchet, R. (2024). Tuning Ceramic Surface to Minimize the Ionic Resistance at the Interface between PEO- and LATP-Based Ceramic Electrolyte. ACS Applied Materials & Interfaces, 16(34), 45713-45723. https://doi.org/10.1021/acsami.4c08882
Vancouver
Mangani LR, Devaux D, Benayad A, Jordy C, Bouchet R. Tuning Ceramic Surface to Minimize the Ionic Resistance at the Interface between PEO- and LATP-Based Ceramic Electrolyte. ACS Applied Materials & Interfaces. 2024;16(34):45713-45723. doi:10.1021/acsami.4c08882
BibTeX
@article{Mangani2024,
author = {Mangani, Léa R and Devaux, Didier and Benayad, Anass and Jordy, Christian and Bouchet, Renaud},
title = {Tuning Ceramic Surface to Minimize the Ionic Resistance at the Interface between PEO- and LATP-Based Ceramic Electrolyte},
journal = {ACS Applied Materials & Interfaces},
year = {2024},
volume = {16},
number = {34},
pages = {45713--45723},
doi = {10.1021/acsami.4c08882}
}
EUVIMED