Synthesis of a Mesoporous SnO 2 Catalyst Support and the Effect of Its Pore Size on the Performance of Polymer Electrolyte Fuel Cells
ACS Applied Materials & Interfaces · 28.02.2024 · 16 (8) · 10295-10306
DOI: 10.1021/acsami.4c01794 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Materials & Interfaces, online erschienen am 21.02.2024. Verfasst von Masanori Inaba und 11 weiteren Autor:innen. Beteiligte Einrichtung: Toyota Central R&D Laboratories., Inc., Nagakute, Aichi 480-1192, Japan. Die Arbeit wurde bisher 39-mal zitiert (Crossref) und nennt 65 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0).
Abstract (Originalsprache)
The aim of this study was to clarify the effectiveness and challenges of applying mesoporous tin oxide (SnO2)-based supports for Pt catalysts in the cathodes of polymer electrolyte fuel cells (PEFCs) to simultaneously achieve high performance and high durability. Recently, the focus of PEFC application in automobiles has shifted to heavy-duty vehicles (HDVs), which require high durability, high energy-conversion efficiency, and high power density. It has been reported that employing mesoporous carbon supports improves the initial performance by mitigating catalyst poisoning caused by sulfonic acid groups of the ionomer as well as by reducing the oxygen transport resistance through the Pt/ionomer interface. However, carbon materials in the cathode can degrade oxidatively during long-term operation, and more stable materials are desired. In this study, we synthesized connected mesoporous Sb-doped tin oxides (CMSbTOs) with controlled mesopore sizes in the range of 4-11 nm and tested their performance and durability as cathode catalyst supports. The CMSbTO supports exhibited higher fuel cell performance at a pore size of 7.3 nm than the solid-core SnO2-based, solid-core carbon, and mesoporous carbon supports under dry conditions, which can be attributed to the mitigation of the formation of the Pt/ionomer interface and the better proton conductivity within the mesopores even at the low-humidity conditions. In addition, the CMSbTO supports exhibited high durability under oxidative conditions. These results demonstrate the promising applicability of mesoporous tin oxide supports in PEFCs for HDVs. The remaining challenges, including the requirements for improving performance under wet conditions and stability under reductive conditions, are also discussed.
Schlagwörter
Stichwörter der Autor:innen
Autor:innen und Institutionen
- Toyota Central R&D Laboratories., Inc., Nagakute, Aichi 480-1192, Japan.
- Toyota Motor Corporation, Susono,Shizuoka410-1193, Japan.
ORCID-Profile: Masanori Inaba, Noritake Isomura, Wataru Yoshimune, Kensaku Kodama
Zitieren
APA
Inaba, M., Murase, R., Takeshita, T., Yano, K., Kosaka, S., Takahashi, N., Isomura, N., Oh-Ishi, K., Yoshimune, W., Tsuchiya, K., Nobukawa, T., & Kodama, K. (2024). Synthesis of a Mesoporous SnO 2 Catalyst Support and the Effect of Its Pore Size on the Performance of Polymer Electrolyte Fuel Cells. ACS Applied Materials & Interfaces, 16(8), 10295-10306. https://doi.org/10.1021/acsami.4c01794
Vancouver
Inaba M, Murase R, Takeshita T, Yano K, Kosaka S, Takahashi N, et al. Synthesis of a Mesoporous SnO 2 Catalyst Support and the Effect of Its Pore Size on the Performance of Polymer Electrolyte Fuel Cells. ACS Applied Materials & Interfaces. 2024;16(8):10295-10306. doi:10.1021/acsami.4c01794
BibTeX
@article{Inaba2024,
author = {Inaba, Masanori and Murase, Ryuichi and Takeshita, Tomohiro and Yano, Kazuhisa and Kosaka, Satoru and Takahashi, Naoko and Isomura, Noritake and Oh-Ishi, Keiichiro and Yoshimune, Wataru and Tsuchiya, Kimihiro and Nobukawa, Takeshi and Kodama, Kensaku},
title = {Synthesis of a Mesoporous SnO 2 Catalyst Support and the Effect of Its Pore Size on the Performance of Polymer Electrolyte Fuel Cells},
journal = {ACS Applied Materials & Interfaces},
year = {2024},
volume = {16},
number = {8},
pages = {10295--10306},
doi = {10.1021/acsami.4c01794}
}
EUVIMED