Grafted Chitosan for Dye Removal: Synthesis Cost, Material Efficiency and Reuse Risk
ACS Applied Engineering Materials · 29.10.2026
DOI: 10.1021/acsaenm.6c01272 ↗Kurz gefasst
Fachartikel in der Zeitschrift ACS Applied Engineering Materials, online erschienen am 29.10.2026. Verfasst von Despina A. Gkika und 1 weiteren Autor:innen. Die Arbeit nennt 59 Literaturangaben. Der Volltext ist frei zugänglich (Open Access, CC BY-NC-ND 4.0). Gefördert von: Hellenic Academic Libraries Link.
Abstract (Originalsprache)
The economic viability of chitosan-based adsorbents depends on laboratory-scale synthesis costs, adsorption performance, regeneration behavior and synthesis-route complexity. However, these factors are rarely evaluated within a unified framework, limiting informed material selection. Herein, an integrated framework combining activity-based costing and total cost of ownership (ABC−TCO), cost-effectiveness analysis, material-use efficiency and complexity-adjusted risk−return assessment was developed. Four chitosan derivatives, chitosan grafted with acrylic acid (Ch-g-Aa) or acrylamide (Ch-g-Aam) in powder and bead forms, were systematically evaluated for Remazol Yellow Gelb 3RS (RY) and Basic Yellow 37 (BY) removal over four consecutive adsorption−desorption cycles. The results revealed that bead formation improved cost-effectiveness for Ch-g-Aa but reduced it for Ch-g-Aam. Notably, the lowest synthesis cost (€14.35 g−1, Ch-g-Aa beads) did not correspond to the lowest synthesis cost per mg of RY removed: Ch-g-Aa beads incurred 2.6 times the cost of Ch-g-Aam powder (0.01085 versus 0.00423 € mg−1). To assess synthesis-route efficiency, complexity-adjusted risk−return analysis demonstrated that Ch-g-Aa beads achieved the highest economic return (39.01%) and return-to-risk ratio (5.02), despite requiring nine synthesis steps versus six for powders. Raw materials consistently dominated synthesis costs (>60% of batch costs for powders), identifying reagent optimization and solvent recovery as key priorities for synthesis optimization. Overall, bead formation provided no universal advantage; its value depended on graft chemistry, synthesis yield and target pollutant. The framework delivers three benefits: it distinguishes synthesis cost from cost-effectiveness, revealing overlooked trade-offs; identifies when additional synthesis complexity is economically justified; and pinpoints cost and material-use hotspots to guide polymeric adsorbent design.
Förderung
- Hellenic Academic Libraries Link
Zitieren
APA
Gkika, D. A., & Kyzas, G. Z. (2026). Grafted Chitosan for Dye Removal: Synthesis Cost, Material Efficiency and Reuse Risk. ACS Applied Engineering Materials. https://doi.org/10.1021/acsaenm.6c01272
Vancouver
Gkika DA, Kyzas GZ. Grafted Chitosan for Dye Removal: Synthesis Cost, Material Efficiency and Reuse Risk. ACS Applied Engineering Materials. 2026. doi:10.1021/acsaenm.6c01272
BibTeX
@article{Gkika2026,
author = {Gkika, Despina A. and Kyzas, George Z.},
title = {Grafted Chitosan for Dye Removal: Synthesis Cost, Material Efficiency and Reuse Risk},
journal = {ACS Applied Engineering Materials},
year = {2026},
doi = {10.1021/acsaenm.6c01272}
}
EUVIMED