Capacity–Retention Balance Determines Single-Crystal Payoff in Ni-Rich Cathodes

Zenghua Tian, Huazhang Zhou, Mingle Chu, Sainan Yao, Xudong Li, Yongming Zhu

ACS Applied Energy Materials · 09.11.2026 · 9 (21) · 14732-14739

DOI: 10.1021/acsaem.6c03137 ↗

Kurz gefasst

Fachartikel in der Zeitschrift ACS Applied Energy Materials, online erschienen am 26.10.2026. Verfasst von Zenghua Tian und 5 weiteren Autor:innen. Die Arbeit nennt 31 Literaturangaben. Gefördert von: National Natural Science Foundation of China, Natural Science Foundation of Shandong Province.

AbstractBibliografische AngabenZitierenVerwandte Studien

Abstract (Originalsprache)

Single crystallization is widely pursued to mitigate structural degradation in Ni-rich layered cathodes, yet its practical value remains difficult to define because improved durability can be accompanied by kinetic limitations and an initial-capacity penalty. Here, we establish a literature-derived quantitative framework that converts this long-standing trade-off into a measurable payoff criterion. Directly comparable polycrystalline–single-crystal cathode pairs from 12 datasets and 42 test contexts were evaluated through logarithmic response ratios describing initial-capacity, retention, and end-of-test capacity effects. Single-crystal cathodes showed higher retention in 67% of comparisons but higher initial capacity in only 19%, while 64% ultimately achieved a higher end-of-test capacity. These results identify compensation between early capacity sacrifice and durability gain as the central determinant of single-crystal benefit. Cross-dataset analysis further shows that this payoff is condition-dependent. The resulting break-even framework shifts single crystallization from a qualitative stability preference to a quantitative materials selection principle and offers a broader strategy for evaluating energy-storage materials in which long-term durability is gained at the expense of initial performance.

Förderung

  • National Natural Science Foundation of China
  • Natural Science Foundation of Shandong Province

Zitieren

APA

Tian, Z., Zhou, H., Chu, M., Yao, S., Li, X., & Zhu, Y. (2026). Capacity–Retention Balance Determines Single-Crystal Payoff in Ni-Rich Cathodes. ACS Applied Energy Materials, 9(21), 14732-14739. https://doi.org/10.1021/acsaem.6c03137

Vancouver

Tian Z, Zhou H, Chu M, Yao S, Li X, Zhu Y. Capacity–Retention Balance Determines Single-Crystal Payoff in Ni-Rich Cathodes. ACS Applied Energy Materials. 2026;9(21):14732-14739. doi:10.1021/acsaem.6c03137

BibTeX
@article{Tian2026,
  author = {Tian, Zenghua and Zhou, Huazhang and Chu, Mingle and Yao, Sainan and Li, Xudong and Zhu, Yongming},
  title = {Capacity–Retention Balance Determines Single-Crystal Payoff in Ni-Rich Cathodes},
  journal = {ACS Applied Energy Materials},
  year = {2026},
  volume = {9},
  number = {21},
  pages = {14732--14739},
  doi = {10.1021/acsaem.6c03137}
}
Kostenlos starten →