Leaching kinetic mechanism of iron from the diamond wire saw silicon powder by HCl
Waste Management · 2023-09 · 169 · 82-90
DOI: 10.1016/j.wasman.2023.06.028 ↗Kurz gefasst
Fachartikel in der Zeitschrift Waste Management, 2023-09. Verfasst von Zhaoyang Zhang und 7 weiteren Autor:innen. Beteiligte Einrichtung: Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China; School of Materia…. Hauptthemen laut MEDLINE: Iron, Silicon. Die Arbeit wurde bisher 33-mal zitiert (Crossref) und nennt 37 Literaturangaben. Gefördert von: National Natural Science Foundation of China, National Key Research and Development Program of China.
Abstract (Originalsprache)
The diamond wire saw silicon powder (DWSSP) is considered to be a harmful to the environment because of finer particles, the large specific surface area and flammability. Removal of Fe impurity is very essential for recovering Si from DWSSP due to the large amount of Fe introduced during the silicon powder generation process. In the study, the thermodynamics of Fe leaching with HCl was analyzed and determined iron was theoretically present as ions in solution. Furthermore, the effects of different concentrations, temperatures and liquid-solid ratios on Fe leaching from HCl were investigated. The leaching rate of Fe reached 98.37% at the optimal parameters (HCl concentration of 12 wt%, leaching temperature of 333 K, liquid-solid ratio of 15 ml/g) with 100 min. The leaching kinetics of Fe in HCl was analyzed by shrinking core model and homogeneous model, respectively. The study indicated the process of leaching Fe from DWSSP conforms to the secondary reaction model of homogeneous model which coincided with the porous structure of DWSSP due to agglomeration. The apparent activation energy required (49.398 kJ/mol) in the first stage is lower than that (57.817 kJ/mol) in the second stage because of the porous structure. In conclusion, this paper provided a suitable way to purify the diamond wire saw silicon powder. This work provides an important guide for the industrial recovery and preparation of high purity silicon from DWSSP by the most environment-friendly and low-cost approach.
Schlagwörter
MeSH-Schlagwörter (MEDLINE)
Stichwörter der Autor:innen
Substanzen
Autor:innen und Institutionen
- Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China; School of Materials and Engineering, Northeastern University, Shenyang 110819, China.
- School of Metallurgy, Northeastern University, Shenyang 110819, China.
- Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819, China; School of Materials and Engineering, Northeastern University, Shenyang 110819, China. E…
- School of Metallurgy, Northeastern University, Shenyang 110819, China. Electronic address: Xingpf@smm.neu.edu.cn.
Förderung
- National Natural Science Foundation of China
- National Key Research and Development Program of China
Zitieren
APA
Zhang, Z., Guo, X., Wang, Y., Wei, D., Wang, H., Li, H., Zhuang, Y., & Xing, P. (2023). Leaching kinetic mechanism of iron from the diamond wire saw silicon powder by HCl. Waste Management, 169, 82-90. https://doi.org/10.1016/j.wasman.2023.06.028
Vancouver
Zhang Z, Guo X, Wang Y, Wei D, Wang H, Li H, et al. Leaching kinetic mechanism of iron from the diamond wire saw silicon powder by HCl. Waste Management. 2023;169:82-90. doi:10.1016/j.wasman.2023.06.028
BibTeX
@article{Zhang2023,
author = {Zhang, Zhaoyang and Guo, Xiaolin and Wang, Yaoxuan and Wei, Donghui and Wang, Hong and Li, Haiyu and Zhuang, Yanxin and Xing, Pengfei},
title = {Leaching kinetic mechanism of iron from the diamond wire saw silicon powder by HCl},
journal = {Waste Management},
year = {2023},
volume = {169},
pages = {82--90},
doi = {10.1016/j.wasman.2023.06.028}
}